Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Nypel® 6235G BK1 - PA6-GF35 - BASF

Material Data Center offers the following functions for Nypel® 6235G BK1:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Nypel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Nypel 6235G BK1 is a 35% glass reinforced injection molding grade of PA6. Based on recycled polyamide feedstocks, Nypel 6235G BK1 offers a balance of mechanical properties with excellent flow and surface appearance.

Nypel 6235G BK1 is recommended for lawn and power equipment housings, structural furniture components such as seat frames, and automotive and industrial applications.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 76 / * cm³/10min ISO 1133
온도 275 / * °C -
하중 5 / * kg -
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 10999 / 7854 MPa ISO 527
파단시 강도 172 / 116 MPa ISO 527
파단시 신율 3.2 / 6.2 % ISO 527
챠피 충격 강도 , +23°C 90 / 104 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 77 / 75 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 17 / 20 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 14 / 14 kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 218 / * °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 207 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 217 / * °C ISO 75-1/-2
기타 특성건조/응축단위시험규격
물에서의 흡수성 1.25 / * % ISO 62와 유사
조건에서의 흡습성 5.1 / * % ISO 62와 유사
밀도 1380 / - kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 °C -
Pre-drying - Time 4 h -
용융수지온도 270 - 290 °C -
성형온도 80 - 90 °C -
특징
생산 공정
사출 성형
인도 유형
검정
Certifications
Recycled Resin Content
응용
자동차의
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Mold temperature, range: 80 - 90 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.