Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Panlite® G-3410R - PC-GF10 - Teijin Chemicals Ltd.

Material Data Center offers the following functions for Panlite® G-3410R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Panlite datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
성형 수축률, 평행 0.004 mm/mm ASTM D 955
성형 수축률, 수직 0.005 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 3700 MPa ISO 527
파단시 강도 70 MPa ISO 527
파단시 신율 3.5 % ISO 527
굴곡 계수, 23°C 3600 MPa ISO 178
굴곡 강도 120 MPa ISO 178
챠피 충격 강도, +23°C 55 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 10 kJ/m² ISO 179/1eA
ASTM 데이터
인장탄성률 3630 MPa ASTM D 638
파단시 강도 76 MPa ASTM D 638
파단시 신율 4 % ASTM D 638
압축 강도 94 MPa ASTM D 695
굴곡 계수 3530 MPa ASTM D 790
굴곡 강도 118 MPa ASTM D 790
로크웰 경도 M 84 - ASTM D 785
아이조드 충격은 노치, 1/8 in 78 J/m ASTM D 256
아이조드 충격은 노치, 1/4 in 78 J/m ASTM D 256
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 144 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 149 °C ISO 75-1/-2
비카트 연화 온도, B 151 °C ISO 306
선형 열팽창 계수, 평행 40 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 60 E-6/K ISO 11359-1/-2
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 0.4 mm -
ASTM 데이터
UL94 난연성 V-2 - UL 94
테스트 두께 0.8 mm -
열팽창 계수, 평행 40 E-6/K ASTM D 696
열팽창 계수, 수직 67 E-6/K ASTM D 696
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.2 - IEC 62631-2-1
상대 유전뮬, 1MHz 3.2 - IEC 62631-2-1
소산 인자, 100Hz 10 E-4 IEC 62631-2-1
소산 인자, 1MHz 90 E-4 IEC 62631-2-1
부피 저항 >1E13 Ohm*m IEC 62631-3-1
표면 저항 >1E15 Ohm IEC 62631-3-2
전기 압력 35 kV/mm IEC 60243-1
CTI 175 - IEC 60112
ASTM 데이터
전기 압력, 단기간의 30 kV/mm ASTM D 149
소산 인자, 60 Hz 0.0008 - ASTM D 150
소산 인자, 1 MHz 0.009 - ASTM D 150
상대 유전율, 60 Hz 3.16 - ASTM D 150
상대 유전율, 1 MHz 3.07 - ASTM D 150
부피 저항 >1E15 Ohm*cm ASTM D 257
아크 저항 100 s ASTM D 495
기타 특성단위시험규격
밀도 1270 kg/m³ ISO 1183
물에서의 흡수성, 평형 0.16 % ASTM D 570
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 120 °C -
Pre-drying - Time >5 h -
용융수지온도 290 - 320 °C -
성형온도 80 - 120 °C -
도표
Fatigue strength , Panlite® G-3410R, PC-GF10, Teijin Chemicals
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특성
Creep Resistance
응용
전기 및 전자
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.