Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pebax® 6333 SA 01 MED - TPA - ARKEMA

Material Data Center offers the following functions for Pebax® 6333 SA 01 MED:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Pebax datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Polyether block amide Pebax® 6333 SA 01 MED resin is a thermoplastic elastomer made of flexible polyether and rigid polyamide.
This grade offers the highest quality and it is specially designed to meet the stringent requirements of the medical applications such as minimally invasive devices.
Pebax® 6333 SA 01 MED resin also offers an excellent combination of properties such as: kink resistance, low friction coefficient and superior dynamic response.
Upon request, letters regarding USP Class VI compliance can be provided.


Main applications:
  • Tubings like angiography and angioplasty catheters
  • Flexible injected parts


Packaging:

This grade is delivered dried in sealed packaging (20 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 307 / 240 MPa ISO 527
항복강도 19 / 18 MPa ISO 527
항복변형률 22 / 22 % ISO 527
파단시 평균신율 >50 / >50 % ISO 527
챠피 노치드 충격 강도, -30°C - / 20 kJ/m² ISO 179/1eA
쇼어 D 경도 58 / * - ISO 7619-1
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 169 / * °C ISO 11357-1/-3
비카트 연화 온도, B 85 / * °C ISO 306
기타 특성건조/응축단위시험규격
물에서의 흡수성 1.1 / * % ISO 62와 유사
조건에서의 흡습성 0.7 / * % ISO 62와 유사
밀도 1010 / - kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 65 - 75 °C -
Pre-drying - Time 4 - 6 h -
용융수지온도 230 - 290 °C -
성형온도 25 - 60 °C -
특징
생산 공정
사출 성형, 기타 압출
인도 유형
펠렛 (입자,알갱이)
특별 특성
가시광선 안정성, 열안정성
Certifications
Medical Grade, US Pharmacopeia Class VI Approved
지역별 검색
기타 정보
사E성

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 230°C / 260°C / 290°C.
- Typical mold temperature : 25 – 60°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
기타 압출

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 210°C / 225°C / 240°C.
- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 65-75°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.