Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PHARMALENE® BC 82 PH BA - (PE-HD) - Versalis S.p.A

Material Data Center offers the following functions for PHARMALENE® BC 82 PH BA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pharmalene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Pharmalene BC 82 PH BA will be bio attributed for 95%.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 흐름성, MFI 0.25 g/10min ISO 1133
온도 190 °C -
负荷 2.16 kg -
기계적 특성단위시험규격
ISO 데이터
항복강도 27 MPa ISO 527
파단시 강도 30 MPa ISO 527
파단시 신율 600 % ISO 527
굴곡 계수, 23°C 1200 MPa ISO 178
쇼어 D 경도 64 - ISO 7619-1
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 132 °C ISO 11357-1/-3
비카트 연화 온도, A 125 °C ISO 306
기타 특성단위시험규격
밀도 954 kg/m³ ISO 1183
Processing Recommendation Extrusion단위시험규격
용융수지온도 195 - 205 °C -
Zone 1 170 - 180 °C -
Zone 2 185 - 195 °C -
특징
생산 공정
기타 압출, 중공 성형
인도 유형
펠렛 (입자,알갱이)
내화학성에
Oxidation Resistance
Certifications
Contains renewable resources, Food contact, Food approval 10/2011, Food approval FDA 21 CFR, Medical Grade, US Pharmacopeia Class VI Approved, ISCC Plus
응용
의료
지역별 검색
짱쨌쨈, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.