Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Pyramid™ CC100 - PEEK-Z60 - Polymics, Ltd.

Material Data Center offers the following functions for Pyramid™ CC100:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pyramid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
For more detailed information, please read our brochure
or contact our representatives in your region.
기계적 특성단위시험규격
ASTM 데이터
인장탄성률 36000 MPa ASTM D 638
파단시 강도 310 MPa ASTM D 638
파단시 신율 1 % ASTM D 638
압축 계수 25000 MPa ASTM D 695
압축 강도 275 MPa ASTM D 695
굴곡 계수 34000 MPa ASTM D 790
로크웰 경도 M 110 - ASTM D 785
쇼어 D 경도 96 - ASTM D 2240
아이조드 충격은 노치, 1/8 in 110 J/m ASTM D 256
열적 특성단위시험규격
ASTM 데이터
UL94 난연성 V-0 - UL 94
DTUL @ 264 psi 300 °C ASTM D 648
녹는점 340 °C ASTM D 3418
유리 전이 온도 143 °C ASTM E 1356
전기적 특성단위시험규격
ASTM 데이터
표면 저항 100 Ohm ASTM D 257
부피 저항 100 Ohm*cm ASTM D 257
기타 특성단위시험규격
물에서의 흡수성, 24hr 0.05 % ASTM D 570
밀도 1500 kg/m³ ASTM D 792
특징
인도 유형
검정
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.