Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® ROTO 11 NATURAL - PA11 - ARKEMA

Material Data Center offers the following functions for Rilsan® ROTO 11 NATURAL:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

PA11-P,RDHL,C12-010


Rilsan® ROTO 11 NATURAL resin is a polyamide 11 powder produced from a renewable source. This natural grade is designed for Rotomolding.

 



ARM Impact Strength:
73 °F    140 ft-lbs
 -40 °F    60 ft-lbs

Mechanical properties:
Testing was performed on rotational molded test specimens.

Main applications:
Rotational molding - Rotomolded tanks.

Packaging:
This grade is delivered in 100 lb drums ready to be processed.




Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 965 / - MPa ISO 527
항복강도 43 / - MPa ISO 527
항복변형률 31 / - % ISO 527
파단시 평균신율 >50 / - % ISO 527
챠피 노치드 충격 강도, +23°C 7.5 / - kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 185 / * °C ISO 11357-1/-3
기타 특성건조/응축단위시험규격
밀도 1050 / 1050 kg/m³ ISO 1183
특징
생산 공정
회전 성형
인도 유형
가루, 자연 색상
부가물
가소제
특별 특성
가시광선 안정성, 열안정성
Certifications
Contains renewable resources
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.