Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Rilsan® BSR 30 - PA11-CF30 - ARKEMA

Material Data Center offers the following functions for Rilsan® BSR 30:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Rilsan datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
PA11, MHLR, 11-140, CF 30
Rilsan® BSR 30 resin is a polyamide 11 produced from a renewable source. Light and rigid, this grade is carbon fiber reinforced and designed for injection molding.

According to ASTM D6866, the biobased carbon content is measured at 62%.

Main applications:
  • Quick connectors

Packaging:
This grade is delivered dried in sealed packaging (25 kg bags) ready to be processed.

Shelf Life:
Two years from the delivery. For any use above this limit, please refer to our technical services.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 12 / * cm³/10min ISO 1133
온도 235 / * °C -
하중 5 / * kg -
성형 수축률, 평행 0 / * % ISO 294-4, 2577
성형 수축률, 수직 0.6 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 - / 16300 MPa ISO 527
파단시 강도 - / 167 MPa ISO 527
파단시 신율 - / 5 % ISO 527
챠피 노치드 충격 강도, +23°C - / 20 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C - / 12 kJ/m² ISO 179/1eA
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 188 / * °C ISO 11357-1/-3
기타 특성건조/응축단위시험규격
밀도 1150 / 1150 kg/m³ ISO 1183
Biobased content 60 % -
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 - 90 °C -
Pre-drying - Time 4 - 6 h -
용융수지온도 260 - 290 °C -
성형온도 70 - 100 °C -
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
증가된 전기전도성, 정전기 방지
Certifications
Contains renewable resources
지역별 검색
기타 정보
사E성

Processing conditions:

- Typical melt temperature (Min / Recommended / Max) : 260°C / 275°C / 290°C.
- Mold temperature : 70 - 100°C

- Drying time and temperature (only necessary for bags opened for more than two hours) : 4-6 hours at 80-90°C.

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.