Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of SINKRAL® B4 Milano - ABS - Versalis S.p.A

Material Data Center offers the following functions for SINKRAL® B4 Milano:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Sinkral datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Symbol according to ISO 1043-1: ABS

Designation: Thermoplastics ISO 2580-ABS 1,EGN,105-04-16-20

Sinkral B 4 Milano is a special grade for extrusion/thermoforming.
Thanks to its low gel content toghether an optimum balance of stiffness and impact resistance, ensures high aesthetic quality of surfaces, partcularly suitable for co-extrusion.
Optimal thermal stability and rheological properties also permit the sheet production of large dimensions.


Applications:

Exstruded and co-exstruded sheets, including thick sheet where high hot draw ratios are required.
Its excellent surface appearance permit the use in a wide range of applications such as furniture, refrigerator, sanitary, automotive and packaging for foodstuff and industrial items.
Also ideal for the extrusion of profiles for furniture industry.

 

Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 4 cm³/10min ISO 1133
온도 220 °C -
하중 10 kg -
용융 밀도 960 kg/m³ -
용융 비열용량 2150 J/(kg K) -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2300 MPa ISO 527
항복강도 45 MPa ISO 527
항복변형률 3 % ISO 527
파단시 평균신율 30 % ISO 527
챠피 충격 강도 , +23°C N kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 140 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 18 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 8 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
유리 전이 온도, 10 °C/min 109 °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 83 °C ISO 75-1/-2
비카트 연화 온도, B 104 °C ISO 306
선형 열팽창 계수, 평행 90 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
Yellow Card 유효한 - -
전기적 특성단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 3.1 - IEC 62631-2-1
소산 인자, 1MHz 150 E-4 IEC 62631-2-1
부피 저항 1E13 Ohm*m IEC 62631-3-1
표면 저항 1E14 Ohm IEC 62631-3-2
전기 압력 30 kV/mm IEC 60243-1
CTI 600 - IEC 60112
기타 특성단위시험규격
물에서의 흡수성 0.6 % ISO 62와 유사
조건에서의 흡습성 0.2 % ISO 62와 유사
밀도 1040 kg/m³ ISO 1183
테스트 견본 생산단위시험규격
ISO 데이터
ISO에 따른 공정 조건 2580 - ISO ....-2
사출성형: 용융수지온도 250 °C ISO 294
사출성형: 금형온도 60 °C ISO 294
사출성형: 사출속도 200 mm/s ISO 294
사출성형: 유지압력 70 MPa ISO 294
도표
점도-변형률 , SINKRAL® B4 Milano, ABS, Versalis
전단-변형률 , SINKRAL® B4 Milano, ABS, Versalis
동전단탄성율-온도 , SINKRAL® B4 Milano, ABS, Versalis
응력-신율 , SINKRAL® B4 Milano, ABS, Versalis
시컨트탄성율-신율 , SINKRAL® B4 Milano, ABS, Versalis
비용적-온도(pvT) , SINKRAL® B4 Milano, ABS, Versalis
비엔탈피/질량-온도(DSC) , SINKRAL® B4 Milano, ABS, Versalis
특징
생산 공정
필름 압출, 외형 압출, 시트 압출, 기타 압출, 중공 성형, 열성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
열안정성
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
기타 정보
필름 압출
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

  Typical processing temperature range:

    Melt temperature           190 - 230 °C

기타 압출
Other  extrusion
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

프로파일 압
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

시트 압
PREPROCESSING

Drying conditions if no venting:

    Drying temperature                80 °C

    Drying time                          2 - 4 h

    Maximum water content         0.2 %



PROCESSING

Typical processing temperature range:

    Melt temperature         190 - 230 °C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.