Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Stylac NF920 - ACS - Asahi Kasei

Material Data Center offers the following functions for Stylac NF920:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Stylac datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 55 cm³/10min ISO 1133
온도 220 °C -
하중 10 kg -
용융 흐름성, MFI 59 g/10min ISO 1133
온도 220 °C -
负荷 10 kg -
ASTM 데이터
성형 수축률, 평행 0.0055 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
항복강도 44 MPa ISO 527
굴곡 계수, 23°C 2550 MPa ISO 178
굴곡 강도 70 MPa ISO 178
챠피 노치드 충격 강도, +23°C 7 kJ/m² ISO 179/1eA
로크웰 경도 R 101 - ISO 2039-2
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 74 °C ISO 75-1/-2
비카트 연화 온도, B 88 °C ISO 306
두께가 h인 제품의 난연성 등급 5V 5VA class IEC 60695-11-20
테스트 두께 2.5 mm -
ASTM 데이터
UL94 난연성 V-0 - UL 94
테스트 두께 1.5 mm -
열팽창 계수, 평행 85 E-6/K ASTM D 696
기타 특성단위시험규격
밀도 1160 kg/m³ ISO 1183
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 70 - 80 °C -
Pre-drying - Time 3 - 4 h -
성형온도 40 - 50 °C -
Zone 1 150 - 180 °C -
Zone 2 150 - 190 °C -
Zone 3 170 - 200 °C -
Nozzle temperature 170 - 200 °C -
특징
생산 공정
사출 성형
특별 특성
난연성
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.