Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Teflon™ PFA 345 - PFA - The Chemours Company

Material Data Center offers the following functions for Teflon™ PFA 345:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Teflon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
Other Standards[S]
용융 흐름성, MFI 5 g/10min ASTM D 3307
S: These properties are reported by the producer according standards that are different to our defaults.
기계적 특성단위시험규격
ASTM 데이터
굴곡 계수 551 MPa ASTM D 790
쇼어 D 경도 55 - ASTM D 2240
Other Standards[S]
인장 강도 27 MPa ASTM D 3307
파단시 신율 300 % ASTM D 3307
S: These properties are reported by the producer according standards that are different to our defaults.
열적 특성단위시험규격
ASTM 데이터
UL94 난연성 V-0 - UL 94
산소지수 95 % ASTM D 2863
Other Standards[S]
녹는점 305 °C ASTM D 4591
Max. Service Temp., Continous 260 °C -
S: These properties are reported by the producer according standards that are different to our defaults.
전기적 특성단위시험규격
ASTM 데이터
전기 압력, 단기간의 80 kV/mm ASTM D 149
소산 인자, 1 MHz 0.0002 - ASTM D 150
상대 유전율, 1 MHz 2.03 - ASTM D 150
부피 저항 1E18 Ohm*cm ASTM D 257
기타 특성단위시험규격
물에서의 흡수성, 24hr 0.03 % ASTM D 570
밀도 2150 kg/m³ ASTM D 792
특징
생산 공정
사출 성형, Pipe/Tube Extrusion, Wire/Cable Extrusion, 기타 압출, 트랜스퍼 성형, Compression Molding
인도 유형
펠렛 (입자,알갱이)
특별 특성
U.V. 안정성 또는 기후 안정성, 열안정성
특성
Creep Resistance, Good Drawdown, Low Smoke, Melt Strength, Thermal Stability, Tribologic Grade
내화학성에
General Chemical Resistance, Environmental Stress Crack Resistance
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com