Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Treva™ TR6021-71 - CAP - Eastman Chemical Co.

Material Data Center offers the following functions for Treva™ TR6021-71:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Treva datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서

Eastman TREVA™ Renew Engineering Bioplastic TR6021-71 Natural is a new cellulose-based engineering bioplastic that offers both high performance and reduced environmental impact. Renew polymers enable a brand to reduce

consumption of fossil feedstock-based plastics, achieve sustainability targets without compromise, and be a fast mover in a growing market for sustainable consumer products.

TREVA is chemically resistant, dimensionally stable, flows well, is BPA-free, and has low birefringence.




Processing/Physical Characteristics단위시험규격
ASTM 데이터
성형 수축률, 평행 0.008 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 1880 MPa ISO 527
항복강도 47 MPa ISO 527
항복변형률 5 % ISO 527
파단시 강도 44 MPa ISO 527
파단시 신율 41 % ISO 527
굴곡 계수, 23°C 1730 MPa ISO 178
굴곡 강도 64 MPa ISO 178
아이조드 충격은 노치, +23°C 25 kJ/m² ISO 180/1A
아이조드 충격은 노치 14 kJ/m² ISO 180/1A
온도 -40 °C -
ASTM 데이터
항복강도 48 MPa ASTM D 638
파단시 강도 48 MPa ASTM D 638
파단시 신율 27 % ASTM D 638
굴곡 계수 2090 MPa ASTM D 790
로크웰 경도 R 101 - ASTM D 785
아이조드 충격은 노치, 1/8 in 192 J/m ASTM D 256
아이조드 충격은 노치, Low-Temperature 105 J/m ASTM D 256
온도 -40 °C -
열적 특성단위시험규격
ASTM 데이터
DTUL @ 66 psi 115 °C ASTM D 648
DTUL @ 264 psi 99 °C ASTM D 648
비카트 연화 온도 130 °C ASTM D 1525
기타 특성단위시험규격
Biobased content 48 % -
물에서의 흡수성, 24hr 2.2 % ASTM D 570
밀도 1220 kg/m³ ASTM D 792
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 75 °C -
Pre-drying - Time 4 h -
용융수지온도 260 °C -
성형온도 85 °C -
Injection speed 30 mm/s -
Maximum residence time 4 min -
특징
생산 공정
사출 성형
특별 특성
투명도
특성
Low Birefringence
내화학성에
General Chemical Resistance
Certifications
Contains renewable resources
응용
IT / 비즈니스 기계, 장난감
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.