Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
This is the free Material Data Center Datasheet of TYMAX™ GT7000 - EMA - Westlake Chemical Corp.
unit conversion, PDF datasheet print, comparison with other plastics
Check here, which other Tymax datasheets, application examples or technical articles are available in Material Data Center
Blown and cast films
Tie-layer
TYMAX® GT7000 is a maleic anhydride modified ethylene methyl acrylate copolymer designed for blown and cast film applications. It has a high level of maleic anhydride modification to allow it to be utilized for blending in tailor-made tie layers for multilayer film applications. This resin is designed for bonding to polyolefins, polyamides, EVOH, and PET film layers. It does not contain any slip or antiblock additives.
This product has some 21 CFR clearances.
Processing/Physical Characteristics | 값 | 단위 | 시험규격 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM 데이터 | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
용융 흐름성, MFI | 10 | g/10min | ASTM D 1238 |
열적 특성 | 값 | 단위 | 시험규격 | ||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
ASTM 데이터 | |||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||||
녹는점 | 75 | °C | ASTM D 3418 |
기타 특성 | 값 | 단위 | 시험규격 |
밀도 | 951 | kg/m³ | ASTM D 792 |
Processing Recommendation Extrusion | 값 | 단위 | 시험규격 |
Type of extrusion | blown | - | - |
용융수지온도 | 180 - 200 | °C | - |