Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 4520 FC R01 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 4520 FC R01:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Ultradur® B4520 FC R01 UN is suitable for plastic parts, where material approval direct food contact is a mandatory requirement.

The BASF Ultradur® FC (Food Contact) grades enable the industry to develop products for food contact applications which are in compliance with multiple regional food contact regulations including European Food Contact (EU) Nr. 10/2011 and GMP (EC) N°2023/2006.

For questions regarding the compliance with further regulations, and certificates, please contact your local BASF representative or Plastics Safety (E-Mail: plastics.safety@basf.com).

The products can also be offered as BMBcert™ and/or Ccycled™. Due to the Massbalance approach the product properties do not change.
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 24 cm³/10min ISO 1133
온도 250 °C -
하중 2.16 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2500 MPa ISO 527
항복강도 56 MPa ISO 527
항복변형률 3.6 % ISO 527
파단시 평균신율 >50 % ISO 527
챠피 충격 강도 , +23°C 260 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 200 kJ/m² ISO 179/1eU
Type of failure C - -
챠피 노치드 충격 강도, +23°C 3.5 kJ/m² ISO 179/1eA
Type of failure C - -
챠피 노치드 충격 강도, -30°C 3 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 223 °C ISO 11357-1/-3
하중하에서의 변형온도, 0.45 MPa 130 °C ISO 75-1/-2
기타 특성단위시험규격
밀도 1300 kg/m³ ISO 1183
물질의 비성질단위시험규격
ISO 데이터
점도수 120 cm³/g ISO 307, 1157, 1628
특징
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 70 °C
injection molding, Mold temperature, recommended: 60 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.