Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultradur® B 6550 - PBT - BASF

Material Data Center offers the following functions for Ultradur® B 6550:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultradur datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
High viscosity extrusion grade of fibre optical cable sheaths for semi-finished products, profile and hollow rods in technical applications.

Abbreviated designation according to ISO 1043-1: PBT
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 9 cm³/10min ISO 1133
온도 250 °C -
하중 2.16 kg -
성형 수축률, 평행 1.7 % ISO 294-4, 2577
성형 수축률, 수직 2.1 % ISO 294-4, 2577
ASTM 데이터
성형 수축률, 평행 0.015 mm/mm ASTM D 955
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2400 MPa ISO 527
항복강도 54 MPa ISO 527
항복변형률 3.5 % ISO 527
파단시 평균신율 >50 % ISO 527
탄성변형률, 1h 1800 MPa ISO 899-1
탄성변형률, 1000h 1100 MPa ISO 899-1
챠피 충격 강도 , +23°C N kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 250 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 6 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 3.5 kJ/m² ISO 179/1eA
ASTM 데이터
인장탄성률 2482 MPa ASTM D 638
항복강도 60 MPa ASTM D 638
항복변형률 3.5 % ASTM D 638
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 223 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 55 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 135 °C ISO 75-1/-2
선형 열팽창 계수, 평행 110 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 110 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.5 mm -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 0.8 mm -
ASTM 데이터
DTUL @ 66 psi 135 °C ASTM D 648
DTUL @ 264 psi 53.9 °C ASTM D 648
녹는점 223 °C ASTM D 3418
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.3 - IEC 62631-2-1
상대 유전뮬, 1MHz 3.3 - IEC 62631-2-1
소산 인자, 100Hz 10 E-4 IEC 62631-2-1
소산 인자, 1MHz 200 E-4 IEC 62631-2-1
부피 저항 >1E13 Ohm*m IEC 62631-3-1
표면 저항 1E13 Ohm IEC 62631-3-2
CTI 600 - IEC 60112
기타 특성단위시험규격
물에서의 흡수성 0.5 % ISO 62와 유사
조건에서의 흡습성 0.25 % ISO 62와 유사
밀도 1300 kg/m³ ISO 1183
밀도 1300 kg/m³ ASTM D 792
물질의 비성질단위시험규격
ISO 데이터
점도수 160 cm³/g ISO 307, 1157, 1628
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 80 - 120 °C -
Pre-drying - Time 4 h -
Processing humidity ≤0.04 % -
용융수지온도 250 - 275 °C -
성형온도 40 - 80 °C -
도표
점도-변형률 , Ultradur® B 6550, PBT, BASF
전단-변형률 , Ultradur® B 6550, PBT, BASF
응력-신율 , Ultradur® B 6550, PBT, BASF
시컨트탄성율-신율 , Ultradur® B 6550, PBT, BASF
응력-신율(등시) 23°C, Ultradur® B 6550, PBT, BASF
크립탄성율-시간 23°C, Ultradur® B 6550, PBT, BASF
곡선 크리프 23°C, Ultradur® B 6550, PBT, BASF
인장탄성율-온도 , Ultradur® B 6550, PBT, BASF
특징
생산 공정
사출 성형, 필름 압출, 외형 압출, 시트 압출, 기타 압출
인도 유형
펠렛 (입자,알갱이), 자연 색상
특별 특성
가시광선 안정성, U.V. 안정성 또는 기후 안정성, 열안정성
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 250 - 275 °C
injection molding, Melt temperature, recommended: 260 °C
injection molding, Mold temperature, range: 40 - 80 °C
injection molding, Mold temperature, recommended: 60 °C
injection molding, Dwell time, thermoplastics: 10 min
기타 압출
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Prepreg, Melt temperature: 230 - 250 °C
Extrusion, Pipes, Melt temperature: 230 - 260 °C
Extrusion, cable sheathing, Melt temperature: 230 - 260 °C
프로파일 압
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Profiles, Melt temperature: 230 - 260 °C
시트 압
PREPROCESSING
Pre/Post-processing, max. allowed water content: .04 %
Pre/Post-processing, Pre-drying, Temperature: 80 - 120 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
Extrusion, Plates, Melt temperature: 230 - 250 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com