Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® H2320 008 AT - POM - BASF

Material Data Center offers the following functions for Ultraform® H2320 008 AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
High-molecular-weight grade with somewhat increased flowability for injection molding of relatively thick-walled moldings.

Abbreviated designation according to ISO 1043-1: POM
Designation according to ISO 29988-POM-K,,M-GNR,1-2
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 2.9 cm³/10min ISO 1133
온도 190 °C -
하중 2.16 kg -
성형 수축률, 평행 2.1 % ISO 294-4, 2577
성형 수축률, 수직 2.1 % ISO 294-4, 2577
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2600 MPa ISO 527
항복강도 62 MPa ISO 527
항복변형률 11 % ISO 527
파단시 평균신율 30 % ISO 527
탄성변형률, 1h 1800 MPa ISO 899-1
탄성변형률, 1000h 1300 MPa ISO 899-1
챠피 충격 강도 , +23°C 270 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 260 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 6.5 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 5.5 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 165 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 95 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 156 °C ISO 75-1/-2
비카트 연화 온도, B 150 °C ISO 306
선형 열팽창 계수, 평행 120 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.6 mm -
Yellow Card 유효한 - -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 0.8 mm -
Yellow Card 유효한 - -
산소지수로서의 난연성 15 % ISO 4589-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.8 - IEC 62631-2-1
상대 유전뮬, 1MHz 3.8 - IEC 62631-2-1
소산 인자, 100Hz 10 E-4 IEC 62631-2-1
소산 인자, 1MHz 50 E-4 IEC 62631-2-1
부피 저항 1E11 Ohm*m IEC 62631-3-1
표면 저항 1E13 Ohm IEC 62631-3-2
전기 압력 40 kV/mm IEC 60243-1
CTI 600 - IEC 60112
기타 특성단위시험규격
물에서의 흡수성 0.95 % ISO 62와 유사
조건에서의 흡습성 0.25 % ISO 62와 유사
밀도 1410 kg/m³ ISO 1183
도표
비용적-온도(pvT) , Ultraform® H2320 008 AT, POM, BASF
특징
생산 공정
사출 성형, 필름 압출, 외형 압출, 시트 압출, 기타 압출
인도 유형
펠렛 (입자,알갱이)
부가물
이형제
특성
Copolymer
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 230 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 120 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min
필름 압출
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
Extrusion, Blown film, Melt temperature: 175 - 180 °C
Extrusion, Flat film, Melt temperature: 175 - 180 °C

Processing

Ultraform can be processed to particular advantage using three-section screws having a total length L of 20 - 25 D and a constant pitch of about 1 D. However short-compression zone screws may also be used.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.

Postprocessing

Due to the different solidification and cooling of the melt which varies according to time and place stresses may arise, especially in the case of large wall thicknesses. These stresses can be removed by subsequent heat treatment. Tempering is essential when high demands are placed on dimensional stability. It can be carried out in air, liquid wax or oil at temperatures of 130 - 150, usually 140 - 145 °C. Lower temperatures are not effective. Duration: 10 minutes per 1 mm wall thickness.
기타 압출
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
Extrusion, Prepreg, Melt temperature: 175 - 180 °C
Extrusion, Pipes, Melt temperature: 175 - 180 °C
Extrusion, cable sheathing, Melt temperature: 175 - 180 °C

Processing

Ultraform can be processed to particular advantage using three-section screws having a total length L of 20 - 25 D and a constant pitch of about 1 D. However short-compression zone screws may also be used.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.

Postprocessing

Due to the different solidification and cooling of the melt which varies according to time and place stresses may arise, especially in the case of large wall thicknesses. These stresses can be removed by subsequent heat treatment. Tempering is essential when high demands are placed on dimensional stability. It can be carried out in air, liquid wax or oil at temperatures of 130 - 150, usually 140 - 145 °C. Lower temperatures are not effective. Duration: 10 minutes per 1 mm wall thickness.
프로파일 압
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
Extrusion, Profiles, Melt temperature: 175 - 180 °C

Processing

Ultraform can be processed to particular advantage using three-section screws having a total length L of 20 - 25 D and a constant pitch of about 1 D. However short-compression zone screws may also be used.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.

Postprocessing

Due to the different solidification and cooling of the melt which varies according to time and place stresses may arise, especially in the case of large wall thicknesses. These stresses can be removed by subsequent heat treatment. Tempering is essential when high demands are placed on dimensional stability. It can be carried out in air, liquid wax or oil at temperatures of 130 - 150, usually 140 - 145 °C. Lower temperatures are not effective. Duration: 10 minutes per 1 mm wall thickness.
시트 압
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
Extrusion, Plates, Melt temperature: 175 - 180 °C

Processing

Ultraform can be processed to particular advantage using three-section screws having a total length L of 20 - 25 D and a constant pitch of about 1 D. However short-compression zone screws may also be used.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.

Postprocessing

Due to the different solidification and cooling of the melt which varies according to time and place stresses may arise, especially in the case of large wall thicknesses. These stresses can be removed by subsequent heat treatment. Tempering is essential when high demands are placed on dimensional stability. It can be carried out in air, liquid wax or oil at temperatures of 130 - 150, usually 140 - 145 °C. Lower temperatures are not effective. Duration: 10 minutes per 1 mm wall thickness.
화학적 매체에 대한 저항력
에서의 아세트산 (질량 5%) (23°C)
23 °C에서의 락트산 (질량 10%) (23°C)
에서의 염산 (질량 36%) (23°C)
23 °C에서의 질산 (질량 40%) (23°C)
에서의 황산 (질량 38%) (23°C)
에서의 황산 (질량 5%) (23°C)
에서의 크롬산 용액 (질량 40%) (23°C)
염기
에서의 수산화나트륨 용액 (질량 35%) (23°C)
에서의 수산화나트륨 용액 (질량 1%) (23°C)
에서의 수산화암모늄 용액 (질량 10%) (23°C)
알코올
23 °C에서의 이소프로필 알코올 (23°C)
23 °C에서의 메탄올 (23°C)
23 °C에서의 에탄올 (23°C)
탄화수소
에서의 n-헥산 (23°C)
에서의 톨루엔 (23°C)
에서의 이소옥탄 (23°C)
케톤
에서의 아세톤 (23°C)
에테르
에서의 디에틸 에테르 (23°C)
광유
에서의 SAE 10W40 멀티그레이드 모터 오일 (130°C)
에서의 SAE 80/90 하이포이드 기어 오일 (130°C)
표준 연료
에서의 ISO 1817 액체 1 (60°C)
에서의 ISO 1817 액체 2 (60°C)
60 °C에서의 ISO 1817 액체 3 (60°C)
에서의 ISO 1817 액체 4 (60°C)
에서의 무알코올 표준 연료 (ISO 1817 액체 C 참조) (23°C)
에서의 알코올성 표준 연료 (ISO 1817 액체 4 참조) (23°C)
에서의 디젤 연료 (ISO 1817 액체 F 참조) (23°C)
에서의 디젤 연료 (ISO 1817 액체 F 참조) (>90°C)
염액
에서의 염화나트륨 용액 (질량 10%) (23°C)
에서의 차아염소산나트륨 용액 (질량 10%) (23°C)
에서의 탄산나트륨 용액 (질량 20%) (23°C)
에서의 탄산나트륨 용액 (질량 2%) (23°C)
기타
에서의 초산 에틸 (23°C)
에서의 과산화수소 (23°C)
에서의 DOT No. 4 브레이크 오일 (130°C)
에서의 에틸렌 글리콜 수용액 (질량 50%) (108°C)
에서의 50% 올레산 + 50% 올리브 오일 (23°C)
에서의 물 (23°C)
에서의 탈이온수 (90°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.