Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® N2310 P AT - POM - BASF

Material Data Center offers the following functions for Ultraform® N2310 P AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
General-purpose injection molding grade containing special lubricant. Low frictional coefficient giving extremely low wear in combination with smooth metal surfaces.

Abbreviated designation according to ISO 1043-1: POM
Designation according to ISO 29988-POM-K,,M-GNRS2,3-2
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 7.5 cm³/10min ISO 1133
온도 190 °C -
하중 2.16 kg -
성형 수축률, 평행 2.1 % ISO 294-4, 2577
성형 수축률, 수직 2.1 % ISO 294-4, 2577
이형온도 110 °C -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2600 MPa ISO 527
항복강도 61 MPa ISO 527
항복변형률 10 % ISO 527
파단시 평균신율 31 % ISO 527
탄성변형률, 1h 1800 MPa ISO 899-1
탄성변형률, 1000h 1300 MPa ISO 899-1
챠피 충격 강도 , +23°C 200 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 180 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 6 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 5 kJ/m² ISO 179/1eA
아이조드 충격은 노치, +23°C 6.5 kJ/m² ISO 180/1A
아이조드 충격은 노치 6 kJ/m² ISO 180/1A
온도 -30 °C -
Ball indentation hardness 135 MPa ISO 2039-1
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 166 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 90 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 157 °C ISO 75-1/-2
비카트 연화 온도, B 150 °C ISO 306
선형 열팽창 계수, 평행 110 E-6/K ISO 11359-1/-2
1.5mm 평균두께에서의 난연성 HB class IEC 60695-11-10
테스트 두께 1.6 mm -
Yellow Card 유효한 - -
두께 H인 제품의 난연성 HB class IEC 60695-11-10
테스트 두께 0.8 mm -
Yellow Card 유효한 - -
산소지수로서의 난연성 15 % ISO 4589-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.8 - IEC 62631-2-1
상대 유전뮬, 1MHz 3.8 - IEC 62631-2-1
소산 인자, 100Hz 10 E-4 IEC 62631-2-1
소산 인자, 1MHz 50 E-4 IEC 62631-2-1
부피 저항 1E12 Ohm*m IEC 62631-3-1
표면 저항 1E12 Ohm IEC 62631-3-2
전기 압력 40 kV/mm IEC 60243-1
CTI 600 - IEC 60112
기타 특성단위시험규격
물에서의 흡수성 0.9 % ISO 62와 유사
조건에서의 흡습성 0.2 % ISO 62와 유사
밀도 1410 kg/m³ ISO 1183
Bulk density 850 kg/m³ -
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 200 °C ISO 294
사출성형: 금형온도 90 °C ISO 294
사출성형: 사출속도 200 mm/s ISO 294
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature 100 °C -
Pre-drying - Time 3 h -
Processing humidity ≤0.2 % -
용융수지온도 190 - 230 °C -
성형온도 60 - 120 °C -
도표
점도-변형률 , Ultraform® N2310 P AT, POM, BASF
전단-변형률 , Ultraform® N2310 P AT, POM, BASF
동전단탄성율-온도 , Ultraform® N2310 P AT, POM, BASF
응력-신율(등시) 23°C, Ultraform® N2310 P AT, POM, BASF
응력-신율(등시) 40°C, Ultraform® N2310 P AT, POM, BASF
응력-신율(등시) 80°C, Ultraform® N2310 P AT, POM, BASF
비용적-온도(pvT) , Ultraform® N2310 P AT, POM, BASF
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
부가물
윤활제, 이형제
특성
Tribologic Grade, Copolymer
응용
자동차의
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 230 °C
injection molding, Melt temperature, recommended: 200 °C
injection molding, Mold temperature, range: 60 - 120 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.