Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultraform® W2320 003 PRO TR AT - POM - BASF

Material Data Center offers the following functions for Ultraform® W2320 003 PRO TR AT:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Ultraform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Very free-flowing grade for injection molding with special lubricant to minimize friction,wear, stick-slip and squeaking.

Ultraform® PRO offers a comprehensive service package, which supports customers in product development for the medical technology market.

Additional compliances may also be available. Please contact your local representative or the Ultraplaste Infopoint (E-Mail: ultraplaste.infopoint@basf.com, Telefon: 49 621-60-78780, Fax: 49 621-60-78730).

For notice:
However, BASF has not designed or tested its plastics with respect to all of the special requirements related to their use in medical devices (defined in risk classes I to III according to the European and US Medical Device legislation) and pharmaceutical applications. Therefore BASF makes no warranties, express or implied, concerning the suitability of any BASF plastics for use in any medical device and pharmaceutical applications.

Abbreviated designation according to ISO 1043-1: POM
Designation according to ISO 29988-POM-K,,M-GNRS2,5-2
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 25 cm³/10min ISO 1133
온도 190 °C -
하중 2.16 kg -
성형 수축률, 평행 2.0 % ISO 294-4, 2577
성형 수축률, 수직 1.9 % ISO 294-4, 2577
기계적 특성단위시험규격
ISO 데이터
인장탄성률 2500 MPa ISO 527
항복강도 50 MPa ISO 527
항복변형률 5.5 % ISO 527
파단시 평균신율 37 % ISO 527
챠피 충격 강도 , +23°C 110 kJ/m² ISO 179/1eU
챠피 충격 강도, -30°C 95 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C 5 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, -30°C 4.4 kJ/m² ISO 179/1eA
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 167 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 92 °C ISO 75-1/-2
선형 열팽창 계수, 평행 125 E-6/K ISO 11359-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전율, 100Hz 3.5 - IEC 62631-2-1
상대 유전뮬, 1MHz 3.5 - IEC 62631-2-1
소산 인자, 100Hz 9 E-4 IEC 62631-2-1
소산 인자, 1MHz 55 E-4 IEC 62631-2-1
부피 저항 1E11 Ohm*m IEC 62631-3-1
표면 저항 1E14 Ohm IEC 62631-3-2
CTI 600 - IEC 60112
기타 특성단위시험규격
물에서의 흡수성 0.8 % ISO 62와 유사
조건에서의 흡습성 0.2 % ISO 62와 유사
밀도 1380 kg/m³ ISO 1183
도표
점도-변형률 , Ultraform® W2320 003 PRO TR AT, POM, BASF
전단-변형률 , Ultraform® W2320 003 PRO TR AT, POM, BASF
동전단탄성율-온도 , Ultraform® W2320 003 PRO TR AT, POM, BASF
응력-신율 , Ultraform® W2320 003 PRO TR AT, POM, BASF
시컨트탄성율-신율 , Ultraform® W2320 003 PRO TR AT, POM, BASF
응력-신율(등시) 23°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
크립탄성율-시간 23°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
곡선 크리프 23°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
응력-신율(등시) 40°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
크립탄성율-시간 40°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
곡선 크리프 40°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
응력-신율(등시) 60°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
크립탄성율 -시간 60°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
곡선 크리프 60°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
응력-신율(등시) 80°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
크립탄성율-시간 80°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
곡선 크리프 80°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
응력-신율(등시) 100°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
크립탄성율-시간 100°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
곡선 크리프 100°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
응력-신율(등시) 120°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
크립탄성율- 시간 120°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
곡선 크리프 120°C, Ultraform® W2320 003 PRO TR AT, POM, BASF
비용적-온도(pvT) , Ultraform® W2320 003 PRO TR AT, POM, BASF
인장탄성율-온도 , Ultraform® W2320 003 PRO TR AT, POM, BASF
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
부가물
윤활제, 이형제
특성
Tribologic Grade
응용
의료
지역별 검색
기타 정보
사E성
PREPROCESSING
Pre/Post-processing, max. allowed water content: .2 %
Pre/Post-processing, Pre-drying, Temperature: 100 °C
Pre/Post-processing, Pre-drying, Time: 3 h

PROCESSING
injection molding, Melt temperature, range: 190 - 230 °C
injection molding, Melt temperature, recommended: 210 °C
injection molding, Mold temperature, range: 60 - 120 °C
injection molding, Mold temperature, recommended: 90 °C
injection molding, Dwell time, thermoplastics: 10 min

Processing

Usual single-flighted three-section screws with an effective screw length of at least 15 D, better 20 - 23 D are suitable for the injection molding of Ultraform.

Pretreatment

Granules or pellets in original packaging can be processed without any special pretreatment. Granules or pellets which have become moist due to prolonged or incorrect storage (e.g. by formation of condensed water) must be dried in dehumidifying or recirculating air dryers for approx. 3 hours at about 100 - 110 °C. The moisture content should not exceed 0.2 %.


Postprocessing

If parts were produced at a comparatively low mold temperature (e.g. in order to obtain short cycle times) and must not change their geometry in use thermal postprocessing inducing dimensional changes by postcrystallization may be necessary. In such cases parts should be stored in an oven with recirculated air at temperatures of 100 - 130 °C until dimensions don't change significantly any further. The time needed for this has to be determined experimentally.
화학적 매체에 대한 저항력
에서의 아세트산 (질량 5%) (23°C)
23 °C에서의 락트산 (질량 10%) (23°C)
에서의 염산 (질량 36%) (23°C)
23 °C에서의 질산 (질량 40%) (23°C)
에서의 황산 (질량 38%) (23°C)
에서의 황산 (질량 5%) (23°C)
에서의 크롬산 용액 (질량 40%) (23°C)
염기
에서의 수산화나트륨 용액 (질량 35%) (23°C)
에서의 수산화나트륨 용액 (질량 1%) (23°C)
에서의 수산화암모늄 용액 (질량 10%) (23°C)
알코올
23 °C에서의 이소프로필 알코올 (23°C)
23 °C에서의 메탄올 (23°C)
23 °C에서의 에탄올 (23°C)
탄화수소
에서의 n-헥산 (23°C)
에서의 톨루엔 (23°C)
에서의 이소옥탄 (23°C)
케톤
에서의 아세톤 (23°C)
에테르
에서의 디에틸 에테르 (23°C)
광유
에서의 SAE 10W40 멀티그레이드 모터 오일 (130°C)
에서의 SAE 80/90 하이포이드 기어 오일 (130°C)
표준 연료
에서의 ISO 1817 액체 1 (60°C)
에서의 ISO 1817 액체 2 (60°C)
60 °C에서의 ISO 1817 액체 3 (60°C)
에서의 ISO 1817 액체 4 (60°C)
에서의 무알코올 표준 연료 (ISO 1817 액체 C 참조) (23°C)
에서의 알코올성 표준 연료 (ISO 1817 액체 4 참조) (23°C)
에서의 디젤 연료 (ISO 1817 액체 F 참조) (23°C)
에서의 디젤 연료 (ISO 1817 액체 F 참조) (>90°C)
염액
에서의 염화나트륨 용액 (질량 10%) (23°C)
에서의 차아염소산나트륨 용액 (질량 10%) (23°C)
에서의 탄산나트륨 용액 (질량 20%) (23°C)
에서의 탄산나트륨 용액 (질량 2%) (23°C)
기타
에서의 초산 에틸 (23°C)
에서의 과산화수소 (23°C)
에서의 DOT No. 4 브레이크 오일 (130°C)
에서의 에틸렌 글리콜 수용액 (질량 50%) (108°C)
에서의 50% 올레산 + 50% 올리브 오일 (23°C)
에서의 물 (23°C)
에서의 탈이온수 (90°C)
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.