Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultrafuse PA - PA666 - BASF

Material Data Center offers the following functions for Ultrafuse PA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Ultrafuse datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 49.5 / * cm³/10min ISO 1133
온도 275 / * °C -
하중 5 / * kg -
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 196 / * °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 49 / * °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 65 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 135 / * °C ISO 75-1/-2
비카트 연화 온도, B 172 / * °C ISO 306
기타 특성건조/응축단위시험규격
밀도 1110 / 1050 kg/m³ ISO 1183
3D Data건조/응축단위시험규격
Other Standards[S]
인장탄성률, flat 2420 / 395 MPa ISO 527
인장탄성률, upright 2120 / 334 MPa ISO 527
인장 강도, flat 61.4 / 33.2 MPa ISO 527
인장 강도, upright 16.4 / 17.6 MPa ISO 527
파단시 신율 , flat 9.6 / 143 % ISO 527
파단시 신율 , upright 0.8 / 12.8 % ISO 527
굴곡 계수, flat 2050 / 445 MPa ISO 178
굴곡 계수, on-edge 2250 / 468 MPa ISO 178
굴곡 계수, upright 2150 / 428 MPa ISO 178
굴곡 강도, flat 77 / 17.7 MPa ISO 178
굴곡 강도, on-edge 95.5 / 18.1 MPa ISO 178
굴곡 강도, upright 40.2 / 17.3 MPa ISO 178
챠피 충격 강도 , +23°C, flat 23 / 0 kJ/m² ISO 179/1eU
챠피 충격 강도, +23°C, on-edge 29.7 / 0 kJ/m² ISO 179/1eU
챠피 충격 강도, +23°C, upright 3.5 / 13.4 kJ/m² ISO 179/1eU
챠피 노치드 충격 강도, +23°C, flat 5.6 / - kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, +23°C, on-edge 3.3 / 136 kJ/m² ISO 179/1eA
챠피 노치드 충격 강도, +23°C, upright 1.2 / 9.4 kJ/m² ISO 179/1eA
Izod충격강도, +23°C, flat 28 / 0 kJ/m² ISO 180/1U
Izod충격강도, +23°C, on-edge 45.6 / 0 kJ/m² ISO 180/1U
Izod충격강도, +23°C, upright 3.2 / 17.4 kJ/m² ISO 180/1U
아이조드 충격은 노치, +23°C, flat 5.8 / 85.4 kJ/m² ISO 180/1A
아이조드 충격은 노치, +23°C, on-edge 3.9 / 106 kJ/m² ISO 180/1A
아이조드 충격은 노치, +23°C, upright 1.7 / 10.1 kJ/m² ISO 180/1A
S: These properties are reported by the producer according standards that are different to our defaults.
특징
생산 공정
Additive Manufacturing
인도 유형
Monofilament
특성
Thermal Stability
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com