Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of UNIVAL™ DMDD-6230 NT 7 - (PE-HD) - The Dow Chemical Company

Material Data Center offers the following functions for UNIVAL™ DMDD-6230 NT 7:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Unival datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Processing/Physical Characteristics단위시험규격
ASTM 데이터
용융 흐름성, MFI 0.25 g/10min ASTM D 1238
온도 190 °C -
하중 2.16 kg -
기계적 특성단위시험규격
ASTM 데이터
항복강도 23.4 MPa ASTM D 638
파단시 강도 33.8 MPa ASTM D 638
항복변형률 8 % ASTM D 638
파단시 신율 1000 % ASTM D 638
쇼어 D 경도 60 - ASTM D 2240
열적 특성단위시험규격
ASTM 데이터
DTUL @ 66 psi 66 °C ASTM D 648
비카트 연화 온도 127 °C ASTM D 1525
Other Standards[S]
녹는점 130 °C Dow Method
S: These properties are reported by the producer according standards that are different to our defaults.
기타 특성단위시험규격
밀도 949 kg/m³ ASTM D 792
특징
생산 공정
중공 성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
고충격 또는 고충격 보강, Translucent
특성
Low Odor
내화학성에
General Chemical Resistance, Environmental Stress Crack Resistance
Certifications
Food contact, Food approval 10/2011, Food approval FDA 21 CFR, US Pharmacopeia Class VI Approved, Drug Master File
응용
의료, 포장
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.