Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® i4 R - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® i4 R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Implantable grade polyether ether ketone rod stock for permanent implants

VESTAKEEP® i4 R is a rod stock based on implantable grade neat polyether ether ketone resin VESTAKEEP® i4 G.

Proven Biocompatibility of VESTAKEEP® i-Grades
The extra high purity and extended quality measures make VESTAKEEP® i-grade materials an excellent choice for permanent implants.

The biocompatibility of VESTAKEEP® i4 R has been tested following ISO 10993-1 recommendations for permanent tissue/bone contact and USP Class VI.

VESTAKEEP® i4 R complies to ASTM F2026 “Standard Specification for Polyetheretherketone (PEEK) Polymers for Surgical Implant Applications”.

A summary of biocompatibility test results is available upon request.

Biocompatibility tests available for i4 R


Delivery of VESTAKEEP® i-Grades
VESTAKEEP® i4 R rods are available in different diameters and lengths.
 
Dimensions of VESTAKEEP® i4 R
Diameter Standard length*
6 to 20 mm 3000 mm
25 to 60 mm 2000 mm
70 to 100 mm 1000 mm
* Custom lengths are also available

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
기계적 특성단위시험규격
ISO 데이터
인장탄성률 4000 MPa ISO 527
항복강도 109 MPa ISO 527
항복변형률 4.8 % ISO 527
파단시 평균신율 >50 % ISO 527
열적 특성단위시험규격
ISO 데이터
녹는점, 10°C/min 340 °C ISO 11357-1/-3
하중하에서의 변형온도, 1.80 MPa 155 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 205 °C ISO 75-1/-2
전기적 특성단위시험규격
ISO 데이터
상대 유전뮬, 1MHz 2.8 - IEC 62631-2-1
기타 특성단위시험규격
물에서의 흡수성 0.4 % ISO 62와 유사
조건에서의 흡습성 0.12 % ISO 62와 유사
밀도 1300 kg/m³ ISO 1183
특징
인도 유형
Semifinished product
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
응용
의료
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.