Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAKEEP® DC 4470 R - PEEK - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAKEEP® DC 4470 R:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestakeep datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Gingiva-colored polyether ether ketone for dental applications

VESTAKEEP® DC4470 R is a gingiva-colored polyether ether ketone (PEEK) grade that is especially designed for removable dentures to meet the aesthetic demands of the patient.
 
Biocompatibility of VESTAKEEP® Dental
For VESTAKEEP® DC4470 R, biocompatibility has been tested following ISO 10993-1 recommendations for permanent mucous membrane contact.
The compound composition is optimised for high biocompatibility and superior mechanical, thermal and chemical resistance.
Biocompatibility test reports available for VESTAKEEP® DC4470 R
Standard Description
ISO 10993-03 Genotoxicity: Salmonella Typhimurium Reverse Mutation Test (Ames Test)
ISO 10993-05 Cytotoxicity: Quantitative Growth Inhibition Test
ISO 10993-10 Irritation: Intracutaneous Reactivity
ISO 10993-10 Sensitization: Local Lymph Node Assay
ISO 10993-11 Acute Systemic Toxicity
ISO 10993-11 Subacute / Subchronic Toxicity 14 days
ISO 10993-18 Extraction Tests
USP Class VI Acute Systemic Toxicity Intracutaneous Reactivity Muscle Implantation
Delivery of VESTAKEEP® Dental
VESTAKEEP® DC4470 R rods are available in different diameters and lengths.

Dimensions of VESTAKEEP® DC4470 R
Diameter Standard length
6 and 8 mm 3000 mm
100 mm 1000 mm
Other custom dimensions are available on request.

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.EVONIK.COM/MEDICAL-TECHNOLOGY
기계적 특성단위시험규격
ISO 데이터
인장탄성률 4400 MPa ISO 527
항복강도 110 MPa ISO 527
항복변형률 4.5 % ISO 527
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 155 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 210 °C ISO 75-1/-2
비카트 연화 온도, B 305 °C ISO 306
선형 열팽창 계수, 평행 45 E-6/K ISO 11359-1/-2
기타 특성단위시험규격
물에서의 흡수성 0.4 % ISO 62와 유사
밀도 1360 kg/m³ ISO 1183
특징
인도 유형
Semifinished product
특성
Thermal Stability
내화학성에
General Chemical Resistance
Certifications
Medical Grade, Biocompatibility ISO 10993, US Pharmacopeia Class VI Approved
응용
의료
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.