Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® DX9325 BK E70352 - PA612-GF40 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® DX9325 BK E70352:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Heat-stabilized, glass fiber-reinforced, PA 612 compound for plastic-EPDM-rubber bonds

VESTAMID® DX9325 BK E70352 is a glass fiber-reinforced, PA 612 molding compound. The material contains about 40% glass fiber, an ageing protective agent and processing aid for a fast and even form filling. VESTAMID® DX9325 BK E70352 is especially suitable for the production of plastic and rubber composites. 

Parts of VESTAMID® DX9325 BK E70352 can be co-vulcanized with EPDM-rubbers without using any adhesives or adhesion promoters ("direct-bonding to rubber"). Because of its semi-crystalline morphology VESTAMID® DX9325 BK E70352 provides an excellent chemical resistance, e. g., against greases, oils, fuels and hydraulic fluids.

VESTAMID® DX9325 BK E70352 is supplied as cylindrical pellets ready for processing in moisture-proof bags.

Very important are predrying conditions. The material has to be handle as plasticized PA 612. The drying temperature should be not more than 80°C and the drying time at this temperature not more than 4h.
 
Pigmentation may affect values.

Inside the original and undamaged packaging, the product has a shelf life of at least 2 years when stored in dry rooms at temperatures not exceeding 30°C.

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
OR VISIT OUR PRODUCT AT  WWW.VESTAMID.COM
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
성형 수축률, 평행 0.2 / * % ISO 294-4, 2577
성형 수축률, 수직 0.7 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 10300 / - MPa ISO 527
파단시 강도 160 / - MPa ISO 527
파단시 신율 4.4 / - % ISO 527
챠피 충격 강도 , +23°C 100 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
챠피 충격 강도, -30°C 104 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
챠피 노치드 충격 강도, +23°C 18 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
챠피 노치드 충격 강도, -30°C 16 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
열적 특성건조/응축단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 200 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 215 / * °C ISO 75-1/-2
기타 특성건조/응축단위시험규격
밀도 1410 / - kg/m³ ISO 1183
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 260 °C ISO 294
사출성형: 금형온도 80 °C ISO 294
사출성형: 사출속도 200 mm/s ISO 294
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이), 검정
부가물
이형제
특별 특성
가시광선 안정성, 열안정성
특성
Good Adhesion
내화학성에
General Chemical Resistance, Grease Resistance, Oil Resistance
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.