Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTAMID® Terra HS1851 - PA610-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTAMID® Terra HS1851:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Medium viscosity, glass fiber–reinforced, easily demoldable, heat-stabilized polyamide 610 compound for efficient injection molding

VESTAMID® Terra HS1851 is a glass fiber-reinforced, heat-stabilized, medium-viscosity PA 610 compound for injection molding application. The material contains about 20% glass fibers, an ageing protective agent and processing aid for a fast and even form filling.

The carbonamide groups (-CO-NH-) of the polyamides form hydrogen bridge bonds between the chains of the macromolecules, thereby substantially promoting crystallinity and increasing their strength, melting point, resistance to chemicals and even water absorption. This is characteristic of all semi-crystalline polyamides.

Because of its semi-crystalline morphology VESTAMID® Terra HS1851 provides a high impact strength, excellent chemical resistance (e.g. against greases, oils, alkalis and saline solutions), a low coefficient of friction and high abrasion resistance.
 

VESTAMID® Terra HS1851 is supplied as cylindrical granules, ready for processing, in moisture-proof bags.

 

VESTAMID® Terra is a group of new polyamides, the monomers for which are based entirely or partly on renewable raw materials.
 

VESTAMID® Terra HS is the polycondensation product of 1,6-hexamethylene diamine (H) and 1,10-decanedioic acid (sebacic acid—S). Because sebacic acid is derived from castor oil, VESTAMID® Terra HS is a material that is partly based on bio-based and renewable resources.
 

The use of colorants may affect property values. 

For information about processing of VESTAMID®, please follow the general commendations about “Processing of VESTAMID® compounds”. 

The values presented are typical or average values, they do not constitute a specification.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM OR VISIT OUR PRODUCT AT  WWW.VESTAMID.TERRA.COM
Processing/Physical Characteristics건조/응축단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 21 / * cm³/10min ISO 1133
온도 250 / * °C -
하중 5 / * kg -
성형 수축률, 평행 0.4 / * % ISO 294-4, 2577
성형 수축률, 수직 0.7 / * % ISO 294-4, 2577
기계적 특성건조/응축단위시험규격
ISO 데이터
인장탄성률 6000 / - MPa ISO 527
파단시 강도 131 / - MPa ISO 527
파단시 신율 3.8 / - % ISO 527
챠피 충격 강도 , +23°C 86 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
챠피 충격 강도, -30°C 78 / - kJ/m² ISO 179/1eU
Type of failure C / - - -
챠피 노치드 충격 강도, +23°C 11 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
챠피 노치드 충격 강도, -30°C 8.9 / - kJ/m² ISO 179/1eA
Type of failure C / - - -
열적 특성건조/응축단위시험규격
ISO 데이터
녹는점, 10°C/min 223 / * °C ISO 11357-1/-3
유리 전이 온도, 10 °C/min 49 / * °C ISO 11357-1/-2
하중하에서의 변형온도, 1.80 MPa 204 / * °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 222 / * °C ISO 75-1/-2
비카트 연화 온도, B 219 / * °C ISO 306
선형 열팽창 계수, 평행 26 / * E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 124 / * E-6/K ISO 11359-1/-2
기타 특성건조/응축단위시험규격
물에서의 흡수성 2.6 / * % ISO 62와 유사
밀도 1220 / - kg/m³ ISO 1183
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 260 °C ISO 294
사출성형: 금형온도 80 °C ISO 294
사출성형: 사출속도 200 mm/s ISO 294
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
고충격 또는 고충격 보강, 열안정성
특성
Tribologic Grade
내화학성에
Alkali Resistance, General Chemical Resistance, Grease Resistance, Oil Resistance
Certifications
Contains renewable resources
지역별 검색
쨘횕쩐횈쨍횧쨍짰횆짬, 짱쨌쨈, 쩐횈쩍횄쩐횈 횇횂횈챵쩐챌 횁철쩔짧, 쨀짼쨘횓 쨔횞 횁횩쩐횙 쩐횈쨍횧쨍짰횆짬, 쨉쩔쩐챌 쨔횞 쩐횈횉횁쨍짰횆짬 짹횢쩔짧
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.