Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of VESTORAN® 1900 GF20 HE30018 - PPE-GF20 - Evonik Operations GmbH

Material Data Center offers the following functions for VESTORAN® 1900 GF20 HE30018:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Vestoran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
제품 설명서
Modified polyphenylene ether (PPE), heat resistant, glass fiber-reinforced, suitable for K K process

VESTORAN® 1900GF20 HE30018 is the registered trademark of Evonik Degussa GmbH for molding compounds containing poly-2,6-dimethyl-1,4-phenylene ether as polymeric constituent (polyphenylene ether, PPE, also referred to as PPO).

As a material of amorphous structure VESTORAN® 1900GF20 HE30018 shows very small mold shrinkage. Therefore molded parts have a very low tendency to warp.

Moldings of VESTORAN® 1900GF20 HE30018 are dimensionally stable and hydrolysis resistant even in hot water, but are more sensitive to organic solvents than semi-crystalline plastics.

VESTORAN® 1900GF20 HE30018 is resistant to aqueous alkalines and acides, certain alcohols, and glycol solutions.

Glass fiber reinforcement of this molding material combines outstanding heat deflection temperature under load with high strength and rigidity.

VESTORAN®1900GF20 HE30018 is particularly suitable for the adhesion promoter-free manufacturing of plastic/rubber composites patented K&K process ("direct-bonding to rubber").
 
VESTORAN® 1900GF20 HE30018 is supplied as cylindrical granules in polyethylene packaging.
 
Pigmentation may affect values.

FOR FURTHER INFORMATION PLEASE CONTACT US AT EVONIK-HP@EVONIK.COM
Processing/Physical Characteristics단위시험규격
ISO 데이터
용융 부피 - 흐름 속도, MVR 45 cm³/10min ISO 1133
온도 300 °C -
하중 21.6 kg -
기계적 특성단위시험규격
ISO 데이터
인장탄성률 5700 MPa ISO 527
파단시 강도 103 MPa ISO 527
파단시 신율 2 % ISO 527
챠피 충격 강도 , +23°C 45 kJ/m² ISO 179/1eU
Type of failure C - -
챠피 노치드 충격 강도, +23°C 9 kJ/m² ISO 179/1eA
Type of failure C - -
열적 특성단위시험규격
ISO 데이터
하중하에서의 변형온도, 1.80 MPa 190 °C ISO 75-1/-2
하중하에서의 변형온도, 0.45 MPa 195 °C ISO 75-1/-2
비카트 연화 온도, B 195 °C ISO 306
선형 열팽창 계수, 평행 40 E-6/K ISO 11359-1/-2
선형 열팽창 계수, 수직 50 E-6/K ISO 11359-1/-2
기타 특성단위시험규격
밀도 1200 kg/m³ ISO 1183
특징
생산 공정
사출 성형
인도 유형
펠렛 (입자,알갱이)
특별 특성
열안정성
특성
Amorphous, Good Adhesion, Low Warpage
내화학성에
Acid Resistance, Alkali Resistance, Hydrolytically Stable
지역별 검색
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.