Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Vitane LFC 9585 - TPU - geba Kunststoffcompounds GmbH

Material Data Center offers the following functions for Vitane LFC 9585:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Vitane datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
기계적 특성단위시험규격
ISO 데이터
인장 강도 25 MPa ISO 37
파단시 신율 480 % ISO 37
쇼어 A 경도 85 - ISO 7619-1
Other Standards[S]
10% 변형시 강도 0.35 MPa DIN 53504
100% 변형시 강도 9.5 MPa DIN 53504
S: These properties are reported by the producer according standards that are different to our defaults.
전기적 특성단위시험규격
Other Standards[S]
부피 저항 1E9 Ohm*m IEC 60093
표면 저항 1E12 Ohm IEC 60093
S: These properties are reported by the producer according standards that are different to our defaults.
기타 특성단위시험규격
밀도 1100 kg/m³ ISO 1183
테스트 견본 생산단위시험규격
ISO 데이터
사출성형: 용융수지온도 220 °C ISO 294
사출성형: 금형온도 60 °C ISO 294
Processing Recommendation Injection Molding단위시험규격
Pre-drying - Temperature <80 °C -
Pre-drying - Time 4 - 6 h -
Processing humidity ≤0.02 % -
용융수지온도 210 - 230 °C -
성형온도 40 - 80 °C -
Feed temperature 60 - 80 °C -
Zone 1 210 - 220 °C -
Zone 2 210 - 220 °C -
Zone 3 220 - 230 °C -
Nozzle temperature 220 - 230 °C -
특징
생산 공정
사출 성형
인도 유형
자연 색상
특별 특성
증가된 전기전도성
내화학성에
Oil Resistance
Certifications
Food contact
응용
전기 및 전자 , 포장
지역별 검색
짱쨌쨈
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.