Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of BMC A50 XHS - UP-GF23 - LyondellBasell Industries

Material Data Center offers the following functions for BMC A50 XHS:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other BMC datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Contração após a moldagem, paralelo 0.0025 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Resistência à tração no escoamento 65.5 MPa ASTM D 638
Resistência à compressão 131 MPa ASTM D 695
Módulo de flexão 1241 MPa ASTM D 790
Resistência à flexão 131 MPa ASTM D 790
Dureza Rockwell M75 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 747 J/m ASTM D 256
Impacto Izod com entalhe, 1/4 in 107 J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
UL94 flamabilidade V-0 - UL 94
Espessuras do tubo de teste 1.57 mm -
DTUL @ 66 psi 134 °C ASTM D 648
DTUL @ 264 psi 126 °C ASTM D 648
Temperatura de fusão 218 °C ASTM D 3418
Temp. de transição vítrea 145 °C ASTM E 1356
Temperatura de amolecimento Vicat 151 °C ASTM D 1525
Capacidade térmica específica 1370 J/(kg K) ASTM C 351
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água, 24hr 0.15 % ASTM D 570
Densidade 1890 kg/m³ ASTM D 792
Características
Processamento
Moldagem por injeção
Forma de entrega
Composto de moldagem em massa
Características especiais
Retardante de chama
Disponibilidade regional
América do Norte
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com