BMC - UP - Menzolit
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "BMC" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
Menzolit® BMC 0170 | UP-(MD+GF)73 |
Menzolit® BMC 0200 | UP-(MD+GF)71 |
Menzolit® BMC 0300 | UP-(MD+GF)73 |
Menzolit® BMC 0390 | UP-(MD+GF)75 |
Menzolit® BMC 0400 | UP-(MD+GF)75 |
Menzolit® BMC 0410 | UP-(MD+GF)75 |
Menzolit® BMC 0800 | UP-(MD+GF)73 |
Menzolit® BMC 0900 | UP-(MD+GF)70 |
Menzolit® BMC 1000 | UP-(MD+GF)70 |
Menzolit® BMC 1100 | UP-(MD+GF)69 |
Menzolit® BMC 1400 | UP-(MD+GF)72 |
Menzolit® BMC 1500 | UP-(MD+GF)77 |
Menzolit® BMC 2300 | UP-(MD+GF)64 |
Menzolit® BMC 2500 | UP-(MD+GF)72 |
Menzolit® BMC 2600 | UP-(MD+GF)71 |
Menzolit® BMC 3100 | UP-(MD+GF)77 |
Menzolit® BMC 0190 | UP-(MD+GF) |
Menzolit® BMC 0195 | UP-(MD+GF) |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.