Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Cadence™ GS5 - Copolyester - Eastman Chemical Co.

Material Data Center offers the following functions for Cadence™ GS5:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Cadence datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto

Eastman Cadence™ GS5 is an amorphous copolyester with improved processability for film calendering.

Calendered films made of Eastman Cadence™ copolyester are non-crystallizing, are halogen-free, offer wide calendering and thermoforming windows and have good low-temperature toughness. They are cooperative in secondary operations such as solvent-bonding, lamination, decoration, cold-forming, punching/cutting and mbossment.


Eastman Cadence™ resins require no pre-drying or additional stabilizers.




Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Dureza Shore A 83 - ASTM D 2240
Dureza Shore D 73 - ASTM D 2240
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1270 kg/m³ ASTM D 792
Propriedades do filmeValorUnidadeMétodo de ensaio
ASTM Data
Módulo de tração, long. 1870 MPa ASTM D 882
Módulo de tração, trans. 1820 MPa ASTM D 882
Resistência à tração na ruptura, long. 50 MPa ASTM D 882
Resistência à tração na ruptura, trans. 48 MPa ASTM D 882
Características
Processamento
Calandragem, Termoformagem
Características
Amorfo, Copolímero
Aplicaciones
Embalaje
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.