Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 5201-8 - PC-GX20 - Trinseo

Material Data Center offers the following functions for CALIBRE™ 5201-8:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 8 g/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.3 % ISO 294-4, 2577
ASTM Dados
Índice de fluidez, MFI 8 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.003 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 5170 MPa ISO 527
Tensão no escoamento 83 MPa ISO 527
Deformação no escoamento 2.6 % ISO 527
Tensão na ruptura 83 MPa ISO 527
Deformação na ruptura 3 % ISO 527
Módulo de flexão, 23°C 4820 MPa ISO 178
Impacto Izod com entalhe, +23°C 110 kJ/m² ISO 180/1A
ASTM Dados
Módulo de tração 5171 MPa ASTM D 638
Resistência à tração no escoamento 82.7 MPa ASTM D 638
Resistência à tração na ruptura 82.7 MPa ASTM D 638
Alongamento no escoamento 2.6 % ASTM D 638
Deformação na ruptura 3 % ASTM D 638
Módulo de flexão 4826 MPa ASTM D 790
Resistência à flexão 148 MPa ASTM D 790
Dureza Rockwell R 122 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 107 J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 138 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 158 °C ISO 306
Flamabilidade a 1.5mm esp. nom. V-2 class IEC 60695-11-10
Espessuras do tubo de teste 1.6 mm -
Flamabilidade a espessura h V-0 class IEC 60695-11-10
Espessuras do tubo de teste 3.0 mm -
ASTM Dados
UL94 flamabilidade V-2 - UL 94
Espessuras do tubo de teste 1.59 mm -
DTUL @ 264 psi 138 °C ASTM D 648
Temperatura de amolecimento Vicat 159 °C ASTM D 1525
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1360 kg/m³ ISO 1183
Densidade 1360 kg/m³ ASTM D 792
Características
Aditivos
Desmoldante
Aplicaciones
Elétrica e Eletrônica, Médico
Disponibilidade regional
América do Norte, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.