Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CALIBRE™ 2061-12 - PC - Trinseo

Material Data Center offers the following functions for CALIBRE™ 2061-12:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Calibre datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 12 g/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.6 % ISO 294-4, 2577
ASTM Dados
Índice de fluidez, MFI 12 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.006 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2200 MPa ISO 527
Tensão no escoamento 62.9 MPa ISO 527
Deformação no escoamento 6 % ISO 527
Tensão na ruptura 73.7 MPa ISO 527
Deformação na ruptura >50 % ISO 527
Módulo de flexão, 23°C 2250 MPa ISO 178
Resistência ao impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 46 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 12 kJ/m² ISO 179/1eA
Resistência ao Impacto Izod, +23°C N kJ/m² ISO 180/1U
Impacto Izod com entalhe, +23°C 65 kJ/m² ISO 180/1A
ASTM Dados
Módulo de tração 2220 MPa ASTM D 638
Resistência à tração no escoamento 62.9 MPa ASTM D 638
Alongamento no escoamento 6 % ASTM D 638
Deformação na ruptura 150 % ASTM D 638
Módulo de flexão 2220 MPa ASTM D 790
Resistência à flexão 99.3 MPa ASTM D 790
Dureza Rockwell R118 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 747 J/m ASTM D 256
Resistência ao Impacto Izod, 1/8 in N J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 130 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 147 °C ISO 306
Coef. de expansão térmica linear, paralelo 70 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.5 mm -
Flamabilidade conforme índice de oxigênio 26 % ISO 4589-1/-2
ASTM Dados
UL94 flamabilidade HB - UL 94
Espessuras do tubo de teste 1.5 mm -
Coeficiente de expansão térmica, long. 68.4 E-6/K ASTM D 696
DTUL @ 264 psi 126 °C ASTM D 648
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 3 - IEC 62631-2-1
Constante dielétrica, 1MHz 3 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 10 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 20 E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistência elétrica 17 kV/mm IEC 60243-1
ASTM Dados
Resistência elétrica, tempo curto 16.5 kV/mm ASTM D 149
Fator de dissipação dielétrica, 1 MHz 0.002 - ASTM D 150
Constante dielétrica, 60 Hz 3 - ASTM D 150
Constante dielétrica, 1 MHz 3 - ASTM D 150
Resistividade volumétrica específica >1E15 Ohm*cm ASTM D 257
Propriedades ópticasValorUnidadeMétodo de ensaio
ASTM Dados
Haze 1 % ASTM D 1003
Transmitância luminosa 89 % ASTM D 1003
Índice de refração 1.59 - ASTM D 542
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de umidade 0.32 % Sim. to ISO 62
Densidade 1200 kg/m³ ISO 1183
Absorção de água, 24hr 0.15 % ASTM D 570
Absorção de água, equilíbrio 0.32 % ASTM D 570
Densidade 1200 kg/m³ ASTM D 792
Características
Aditivos
Desmoldante
Características especiais
Alto impacto., Estável contra o calor
Aplicaciones
Médico
Disponibilidade regional
Europa, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.