Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PA66-GF40-02P11/15 - PA66-GLF40 - Celanese

Material Data Center offers the following functions for CELSTRAN® PA66-GF40-02P11/15:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 13700 / 10000 MPa ISO 527
Tensão na ruptura 190 / 160 MPa ISO 527
Deformação na ruptura 1.6 / 2 % ISO 527
Resistência ao impacto Charpy , +23°C 40 / 45 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 41 / - kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 23 / 18 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 23 / - kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 261 / * °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 255 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 8.00 MPa 240 / * °C ISO 75-1/-2
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade - / 1460 kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 80 °C -
Pré-secagem - tempo 4 h -
Temperatura da massa 300 - 315 °C -
Temperatura do molde 90 - 120 °C -
Diagrama
Tensão - deformação , CELSTRAN® PA66-GF40-02P11/15 (dry), PA66-GLF40, Celanese
Tensão - deformação , CELSTRAN® PA66-GF40-02P11/15 (cond.), PA66-GLF40, Celanese
Módulo secante - deformação , CELSTRAN® PA66-GF40-02P11/15 (dry), PA66-GLF40, Celanese
Módulo secante - deformação , CELSTRAN® PA66-GF40-02P11/15 (cond.), PA66-GLF40, Celanese
Características
Processamento
Moldagem por injeção, Extrusão de perfis, Extrusão de chapas, Outros tipos de extrusão, Moldagem por sopro, Moldagem por transferência
Forma de entrega
Granulos
Aditivos
Lubrificantes
Características especiais
Estável contra o calor
Características
Long fiber reinforced
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico
Outras informações
Moldagem por injeção
It is recommended to dry in a dehumidifying dryer: 4 hours at 80 °C.

During the processing of CELSTRAN it is important to watch and
control melt shear, for excessive shear reduces fiber length and
mechanical performance as well.

Processing recommendation:

- Conventional 3 zone screw, screw diameter minimum 40 mm
- Design flow channels for low melt shear
- Back pressure and screw rotation to realize a continous
plastification performance and thus a homogeneous melt.
- Apply higher temperature settings than for short fiber compounds

Melt temperature (in the screw anteroom) 300-315 °C
Mold surface temperature 90-120 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com