Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of CELSTRAN® PP-GF50-0405P10/10 - PP-GLF50 - Celanese

Material Data Center offers the following functions for CELSTRAN® PP-GF50-0405P10/10:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Celstran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 11600 MPa ISO 527
Tensão na ruptura 140 MPa ISO 527
Deformação na ruptura 1.8 % ISO 527
Resistência ao impacto Charpy , +23°C 60 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 58 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 32 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 33 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 165 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 158 °C ISO 75-1/-2
Temperatura de deflexão térmica, 8.00 MPa 138 °C ISO 75-1/-2
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1340 kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 94 °C -
Pré-secagem - tempo 2 h -
Temperatura da massa 260 - 290 °C -
Temperatura do molde 40 - 70 °C -
Diagrama
Tensão - deformação , CELSTRAN® PP-GF50-0405P10/10, PP-GLF50, Celanese
Módulo secante - deformação , CELSTRAN® PP-GF50-0405P10/10, PP-GLF50, Celanese
Características
Processamento
Moldagem por injeção, Extrusão de perfis, Extrusão de chapas, Outros tipos de extrusão, Revestimento, Moldagem por sopro, Moldagem por transferência
Forma de entrega
Granulos
Características especiais
Estável a luz, Estabilidade a raios U.V./Intempéries, Estável contra o calor
Características
Long fiber reinforced
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico
Outras informações
Moldagem por injeção
PP&PE drying requirements: 2 hrs. @94° C.
A dehumidifier or desiccant dryer is recommended.
Celstran can be processed on a standard injection molding unit.
A general purpose metering screw is recommended with a zone
distribution of 40% feed, 40% transition, and 20% metering.
A free flowing check ring assembly is recommended.

Melt Temp: 260-290°C.
Mold Temp: 40- 70°C.
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.