Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Delas 190 - (NBR+PVC) - Lingen Plastic Rubber Co., Ltd.

Material Data Center offers the following functions for Delas 190:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Delas datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Dureza Shore A 90 - ASTM D 2240
Resistência ao rasgamento 42 kN/m ASTM D 624
Resistência à compressão, 22 hr @ 158 °F 65 % ASTM D 395
Resistência à tração 15.5 MPa ASTM D 412
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1260 kg/m³ ASTM D 792
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 60 °C -
Pré-secagem - tempo 4 - 6 h -
Temperatura da massa 170 °C -
Temperatura do molde 30 - 80 °C -
Zona 1 130 - 140 °C -
Zona 2 140 - 160 °C -
Zona 3 160 - 190 °C -
Temperatura do bico 170 - 190 °C -
Velocidade de parafuso 100 - 200 rpm -
Contrapressão 0.05 - 0.5 MPa -
Recomendação de processamento ExtrusãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 60 °C -
Pré-secagem - tempo 4 - 6 h -
Temperatura da massa 160 °C -
Temperatura do molde 150 - 170 °C -
Temperatura - zona de alimentação 130 - 140 °C -
Zona 1 140 - 150 °C -
Zona 2 140 - 150 °C -
Zona 3 150 - 170 °C -
Características
Processamento
Moldagem por injeção, Outros tipos de extrusão
Características especiais
Estabilidade a raios U.V./Intempéries
Resistência Química
Resistência à gordura
Disponibilidade regional
Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.