![Complete Set of CAMPUSĀ® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.](/rev13959/modules/../customized/tradenames/views/images/seo_en.png)
Material datasheets available free. Online registration at: www.materialdatacenter.com
Domolen - PP - DOMO Engineering Plastics
Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.
A search for "Domolen" in Material Data Center leads to the following information:
|
|
Material Data Center offers information about the following products with the requested tradename. To view a datasheet, please click on the relevant product.
Datasheet | Polymer |
---|---|
DOMOLEN PPHT20 BK | PP-T20 |
DOMOLEN PPHT20 NC | PP-T20 |
DOMOLEN PPHG10 NC | PP-GF10 |
DOMOLEN PPHG20 BK | PP-GF20 |
DOMOLEN PPHG20 NC | PP-GF20 |
DOMOLEN PPHT20UV1 BK | PP-T20 |
DOMOLEN PPHT10 NC | PP-T20 |
DOMOLEN PPHLVG30 NC | PP-GF30 |
DOMOLEN PPHLVG30 BK | PP-GF30 |
DOMOLEN PPHLVG30UV1 BK | PP-GF30 |
DOMOLEN PPHHVG30 NC | PP-GF30 |
DOMOLEN PPHHVG30UV1 BK | PP-GF30 |
DOMOLEN PPHHVT20 NC | PP-T20 |
DOMOLEN PPHHVT20H2 NC | PP-T20 |
DOMOLEN PPHHVT20H1 NC | PP-T20 |
DOMOLEN PPHHVG20H2 NC | PP-GF20 |
DOMOLEN PPHHVG35 NC | PP-GF35 |
DOMOLEN PPCG20 BK | PP-GF20 |
DOMOLEN PPCT20 NC | PP-T20 |
DOMOLEN PPCT40 NC | PP-T40 |
DOMOLEN PPCT30 NC | PP-T30 |
DOMOLEN PPCG30 NC | PP-GF30 |
DOMOLEN PPCG40UV1 BK | PP-GF40 |
DOMOLEN PPCG40UV1 NC | PP-GF40 |
DOMOLEN PPCT20UV1 BK | PP-T20 |
DOMOLEN PPCT20UV1 NC | PP-T20 |
DOMOLEN PPCG15UV1 NC | PP-GF15 |
DOMOLEN PPCLVG30 NC | PP-GF30 |
DOMOLEN PPCHVT20 NC | PP-T20 |
Additional information about this tradename, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.
Note: the information in Material Data Center was collected with maximum care, based on information from material producers. They are subject to short term changes at the market. There is no warranty for the correctness of this information. In no way this information can be seen as a legal advice, whether certain tradenames are protected or not.