Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Flomat 516/25 - UP-GF25 - Devi Polymers Private Limited

Material Data Center offers the following functions for Flomat 516/25:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Flomat datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
Other Standards[S]
Contração após a moldagem, paralelo 0.2 % BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Propriedades mecânicasValorUnidadeMétodo de ensaio
Other Standards[S]
Resistência à tração 74 MPa BS-2782
Resistência à flexão 157 MPa BS-2782
Resistência à compressão 177 MPa BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
UL94 flamabilidade V-0 - UL 94
Propriedades elétricasValorUnidadeMétodo de ensaio
ASTM Dados
Resistência ao arco 180 s ASTM D 495
Other Standards[S]
Resistividade volumétrica específica 1E12 Ohm*m DIN 53482
Resistividade superficial específica 1E12 Ohm DIN 53482
Resistência elétrica 12 kV/mm BS 2782
S: These properties are reported by the producer according standards that are different to our defaults.
Outras propriedadesValorUnidadeMétodo de ensaio
Other Standards[S]
Absorção de água 0.2 % BS-2782
Densidade 1800 kg/m³ BS-2782
S: These properties are reported by the producer according standards that are different to our defaults.
Características
Processamento
Moldagem por compressão
Forma de entrega
Composto de moldagem folha
Disponibilidade regional
Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.