Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of GADEL 2200 - PAEK - Gharda Plastics Limited

Material Data Center offers the following functions for GADEL 2200:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Gadel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Contração após a moldagem, paralelo 0.011 mm/mm ASTM D 955
Contração após a moldagem, perpendicular 0.012 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Módulo de tração 4800 MPa ASTM D 638
Resistência à tração 98 MPa ASTM D 638
Deformação na ruptura 4 % ASTM D 638
Módulo de flexão 4700 MPa ASTM D 790
Resistência à flexão 180 MPa ASTM D 790
Dureza Shore D 90 - ASTM D 2240
Impacto Izod com entalhe, 1/8 in 30 J/m ASTM D 256
Resistência ao Impacto Izod, 1/8 in N J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
DTUL @ 264 psi 180 °C ASTM D 648
Temperatura de fusão 385 °C ASTM D 3418
Temp. de transição vítrea 167 °C ASTM E 1356
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1310 kg/m³ ASTM D 792
Características
Características especiais
Estável contra o calor
Resistência Química
Resistência química geral, Resistência a óleos, Resistência à radiação
Aplicaciones
Avião e aeroespacial, Automóvel, Processo químico, Elétrica e Eletrônica
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.