Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HIPEX® HTX9436/38 - TPE - KRAIBURG TPE GmbH & Co. KG

Material Data Center offers the following functions for HIPEX® HTX9436/38:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Hipex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Resistência à tração 8 MPa ISO 37
Deformação na ruptura 410 % ISO 37
Deformação permanente por compressão a 70°C, 24h 54 % ISO 815
Deformação permanente por compressão a 100°C, 24h 51 % ISO 815
Resistência ao rasgamento 25 kN/m ISO 34-1
Dureza Shore A 78 - ISO 7619-1
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1050 kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 105 °C -
Pré-secagem - tempo 2 h -
Umidade do processamento ≤0.1 % -
Temperatura da massa 180 - 220 °C -
Temperatura do molde 40 - 60 °C -
Zona 1 170 °C -
Zona 2 190 °C -
Zona 3 210 °C -
Velocidade de injeção 10 - 20 mm/s -
Pressão de injeção 120 - 200 MPa -
Contrapressão 2 - 10 MPa -
Pressão de recalque 48 - 120 MPa -
Características
Processamento
Moldagem por injeção
Forma de entrega
Cor natural
Características
Boa adesão, Estabilidade térmica
Resistência Química
Resistência à gordura, Resistência a óleos
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.