Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of HOSTAFORM® M25IE - POM - Celanese

Material Data Center offers the following functions for HOSTAFORM® M25IE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Hostaform datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 2.5 cm³/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2400 MPa ISO 527
Tensão no escoamento 61 MPa ISO 527
Deformação no escoamento 11 % ISO 527
Resistência ao impacto Charpy , +23°C 250 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 250 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 8.5 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 163 °C ISO 11357-1/-3
Temperatura de deflexão térmica, 1.80 MPa 91 °C ISO 75-1/-2
Coef. de expansão térmica linear, paralelo 110 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 100 E-6/K ISO 11359-1/-2
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de umidade 0.2 % Sim. to ISO 62
Densidade 1410 kg/m³ ISO 1183
Características
Processamento
Moldagem por injeção, Extrusão de perfis, Extrusão de chapas, Outros tipos de extrusão, Calandragem
Forma de entrega
Granulos
Características
Copolímero
Certifications
Contato com água potável
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Outras informações
Extrusão de perfis
General drying is not necessary due to low moisture absorption of
the resin.

In case of bad storage conditions (water contact or condensed water)
the use of a recirculating air dryer (100 to 120 °C / max. 40 mm
layer / 3 to 6 hours) is recommended.

Max. Water content 0,2 %

Standard extruders with grooved feed zone and short compression
screws (minimum 25 D) will fit.

Melt temperature 180-190 °C



Conditioning e.g. moisturizing is not necessary.

In case of very thick wall thickness profiles after-annealing it is
recommended to reduce internal stress.

Annealing temperature 130-140 °C
Annealing time 10 min/mm thickness
Extrusão de chapas
General drying is not necessary due to low moisture absorption of
the resin.

In case of bad storage conditions (water contact or condensed water)
the use of a recirculating air dryer (100 to 120 °C / max. 40 mm
layer / 3 to 6 hours) is recommended.

Max. Water content 0,2 %

Standard extruders with grooved feed zone and short compression
screws (minimum 25 D) will fit.

Melt temperature 180-190 °C



Conditioning e.g. moisturizing is not necessary.

In case of very thick wall thickness profiles after-annealing it is
recommended to reduce internal stress.

Annealing temperature 130-140 °C
Annealing time 10 min/mm thickness
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com