Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of KOPLA® KDR1031 - PA66-GF - KOPLA CO., LTD

Material Data Center offers the following functions for KOPLA® KDR1031:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kopla datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ASTM Dados
Contração após a moldagem, paralelo 0.006 mm/mm ASTM D 955
Contração após a moldagem, perpendicular 0.0085 mm/mm ASTM D 955
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Resistência ao impacto Charpy, +23°C 97 / 98 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 21 / 26 kJ/m² ISO 179/1eA
ASTM Dados
Módulo de tração 7500 / 5500 MPa ASTM D 638
Resistência à tração 135 / 100 MPa ASTM D 638
Módulo de flexão 6500 / 4900 MPa ASTM D 790
Resistência à flexão 200 / 160 MPa ASTM D 790
Dureza Rockwell R 120 / R 115 - ASTM D 785
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
UL94 flamabilidade HB - UL 94
DTUL @ 66 psi 255 °C ASTM D 648
DTUL @ 264 psi 250 °C ASTM D 648
Temperatura de fusão 260 °C ASTM D 3418
Propriedades elétricasSeco / CondUnidadeMétodo de ensaio
ASTM Dados
Resistência elétrica, tempo curto 34 / - kV/mm ASTM D 149
Fator de dissipação dielétrica, 1 MHz 0.01 / - - ASTM D 150
Constante dielétrica, 1 MHz 3.7 / - - ASTM D 150
Resistividade volumétrica específica 1E15 / - Ohm*cm ASTM D 257
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água, 24hr 0.7 % ASTM D 570
Densidade 1300 kg/m³ ASTM D 792
Características
Características especiais
Alto impacto.
Aplicaciones
Automóvel, Elétrica e Eletrônica
Disponibilidade regional
América do Norte, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.