Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kurarity™ LA3710 - TPE - Kuraray Co., Ltd.

Material Data Center offers the following functions for Kurarity™ LA3710:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Kurarity datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
KURARITY is non-crystalline block copolymer and does not have melting point.
All the KURARITY grades show similar low temperature properties which result from Tg of poly (n-butyl acrylate) or poly (n-butyl acrylate/2-ethylhexyl acrylate) and heat resistance from Tg of PMMA.
LA series : n-butyl acrylate based block copolymers.
Suitable Applications: For PSA.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 11 g/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Res. impacto Charpy c/entalhe, +23°C N kJ/m² ISO 179/1eA
Resistência à tração 3.2 MPa ISO 37
Dureza Shore A 9 - ISO 7619-1
Dureza Shore D 5 - ISO 7619-1
Other Standards[S]
Tensão em 100% de alongamento 0.24 MPa ISO 37
S: These properties are reported by the producer according standards that are different to our defaults.
Propriedades térmicasValorUnidadeMétodo de ensaio
Other Standards[S]
Condutividade térmica, estado sólido 0.14 W/(m K) ASTM E 1530
S: These properties are reported by the producer according standards that are different to our defaults.
Propriedades elétricasValorUnidadeMétodo de ensaio
Other Standards[S]
Fator de dissipação dielétrica, 60 Hz 0.00805 - JIS C 2138
Fator de dissipação dielétrica, 1 MHz 0.00749 - JIS C 2138
Constante dielétrica, 60 Hz 5.01 - JIS C 2138
Constante dielétrica, 1 MHz 4.93 - JIS C 2138
S: These properties are reported by the producer according standards that are different to our defaults.
Propriedades ópticasValorUnidadeMétodo de ensaio
Other Standards[S]
Transmitância luminosa 92 % ISO 13468-1
S: These properties are reported by the producer according standards that are different to our defaults.
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1050 kg/m³ ISO 1183
Características
Forma de entrega
Granulos
Características especiais
Estabilidade a raios U.V./Intempéries, Transparente
Características
Mistura de resina, Boa adesão, Baixo odor, Copolímero
Resistência Química
Resistência a ácidos, Resistência do alcalóide, Resistência a óleos
Aplicaciones
Automóvel, Elétrica e Eletrônica
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.