Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY EF1006FP - PC - LG Chem

Material Data Center offers the following functions for LUPOY EF1006FP:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 17 g/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.7 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.8 % ISO 294-4, 2577
ASTM Dados
Índice de fluidez, MFI 17 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.007 mm/mm ASTM D 955
Contração após a moldagem, perpendicular 0.008 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2100 MPa ISO 527
Tensão no escoamento 58 MPa ISO 527
Deformação no escoamento 6 % ISO 527
Tensão na ruptura 62 MPa ISO 527
Deformação na ruptura 100 % ISO 527
Módulo de flexão, 23°C 2200 MPa ISO 178
Resistência à flexão 89 MPa ISO 178
Res. impacto Charpy c/entalhe, +23°C 20[1] kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 10[1] kJ/m² ISO 179/1eA
Impacto Izod com entalhe, +23°C 17[1] kJ/m² ISO 180/1A
Impacto Izod com entalhe 8[1] kJ/m² ISO 180/1A
Temperatura -30 °C -
Dureza Rockwell R 115 - ISO 2039-2
ASTM Dados
Módulo de tração 2203 MPa ASTM D 638
Resistência à tração no escoamento 60.8 MPa ASTM D 638
Resistência à tração na ruptura 62.8 MPa ASTM D 638
Alongamento no escoamento 6 % ASTM D 638
Deformação na ruptura 110 % ASTM D 638
Módulo de flexão 2178 MPa ASTM D 790
Resistência à flexão 100 MPa ASTM D 790
Dureza Rockwell R 115 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 716 J/m ASTM D 256
Impacto Izod com entalhe, 1/4 in 108 J/m ASTM D 256
Impacto Izod com entalhe, baixa temperatura 98 J/m ASTM D 256
Temperatura -30 °C -
1: 4 mm
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 120[2] °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 134[2] °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 137 °C ISO 306
Coef. de expansão térmica linear, paralelo 74 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 72 E-6/K ISO 11359-1/-2
Flamabilidade a espessura h V-0 class IEC 60695-11-10
Espessuras do tubo de teste 1.0 mm -
Flamabilidade 5V a espessura h 5VB class IEC 60695-11-20
Espessuras do tubo de teste 1.7 mm -
ASTM Dados
UL94 flamabilidade V-0 - UL 94
Espessuras do tubo de teste 1 mm -
Coeficiente de expansão térmica, long. 74 E-6/K ASTM D 696
Coef.de expansão térmica, trans. 72 E-6/K ASTM D 696
DTUL @ 66 psi 136 °C ASTM D 648
DTUL @ 264 psi 123 °C ASTM D 648
Temperatura de amolecimento Vicat 141 °C ASTM D 1525
2: 4 mm
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Resistividade volumétrica específica 1E15 Ohm*m IEC 62631-3-1
Resistividade superficial específica 1E15 Ohm IEC 62631-3-2
Índice comparativo de linha de fuga 212 - IEC 60112
ASTM Dados
Resistência elétrica, tempo curto 20 kV/mm ASTM D 149
Resistividade superficial específica 1E15 Ohm ASTM D 257
Resistividade volumétrica específica 1E17 Ohm*cm ASTM D 257
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de umidade 0.2 % Sim. to ISO 62
Densidade 1180 kg/m³ ISO 1183
Densidade 1180 kg/m³ ASTM D 792
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 100 - 120 °C -
Pré-secagem - tempo 3 - 5 h -
Umidade do processamento ≤0.02 % -
Temperatura da massa 255 - 285 °C -
Temperatura do molde 40 - 80 °C -
Zona 1 240 - 250 °C -
Zona 2 250 - 280 °C -
Zona 3 250 - 280 °C -
Temperatura do bico 250 - 280 °C -
Características
Processamento
Moldagem por injeção
Características especiais
Retardante de chama, Sem halogéneo
Aplicaciones
Automóvel, Elétrica e Eletrônica, Polivalente
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.