Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of LUPOY SP2101F - (PC+SI)-GF10 - LG Chem

Material Data Center offers the following functions for LUPOY SP2101F:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Lupoy datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 10 g/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.6 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.6 % ISO 294-4, 2577
ASTM Dados
Índice de fluidez, MFI 10 g/10min ASTM D 1238
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.006 mm/mm ASTM D 955
Contração após a moldagem, perpendicular 0.006 mm/mm ASTM D 955
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 3570 MPa ISO 527
Tensão no escoamento 50 MPa ISO 527
Deformação no escoamento 5 % ISO 527
Tensão na ruptura 48 MPa ISO 527
Deformação na ruptura 8 % ISO 527
Módulo de flexão, 23°C 3100 MPa ISO 178
Resistência à flexão 85 MPa ISO 178
Res. impacto Charpy c/entalhe, +23°C 17[1] kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 9[1] kJ/m² ISO 179/1eA
Impacto Izod com entalhe, +23°C 15[1] kJ/m² ISO 180/1A
Impacto Izod com entalhe 7[1] kJ/m² ISO 180/1A
Temperatura -40 °C -
Dureza Rockwell R 120 - ISO 2039-2
ASTM Dados
Módulo de tração 3897 MPa ASTM D 638
Resistência à tração no escoamento 54 MPa ASTM D 638
Resistência à tração na ruptura 45.1 MPa ASTM D 638
Alongamento no escoamento 5 % ASTM D 638
Deformação na ruptura 18 % ASTM D 638
Módulo de flexão 2845 MPa ASTM D 790
Resistência à flexão 93.2 MPa ASTM D 790
Dureza Rockwell R 120 - ASTM D 785
Impacto Izod com entalhe, 1/8 in 196 J/m ASTM D 256
Impacto Izod com entalhe, 1/4 in 137 J/m ASTM D 256
Impacto Izod com entalhe, baixa temperatura 88.3 J/m ASTM D 256
Temperatura -30 °C -
1: 4 mm
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 122[2] °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 134[2] °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 138 °C ISO 306
Coef. de expansão térmica linear, paralelo 48 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 77 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espessuras do tubo de teste 1.5 mm -
Flamabilidade a espessura h V-1 class IEC 60695-11-10
Espessuras do tubo de teste 1.0 mm -
ASTM Dados
UL94 flamabilidade HB - UL 94
Espessuras do tubo de teste 0.8 mm -
Coeficiente de expansão térmica, long. 48 E-6/K ASTM D 696
Coef.de expansão térmica, trans. 77 E-6/K ASTM D 696
DTUL @ 66 psi 134[3] °C ASTM D 648
DTUL @ 264 psi 121[3] °C ASTM D 648
Temperatura de amolecimento Vicat 138 °C ASTM D 1525
2: 4 mm  3: 6.4 mm
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Resistividade volumétrica específica 1E15 Ohm*m IEC 62631-3-1
Resistividade superficial específica 1E15 Ohm IEC 62631-3-2
ASTM Dados
Resistência elétrica, tempo curto 19 kV/mm ASTM D 149
Resistividade superficial específica 1E15 Ohm ASTM D 257
Resistividade volumétrica específica 1E17 Ohm*cm ASTM D 257
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de umidade 0.2 % Sim. to ISO 62
Densidade 1240 kg/m³ ISO 1183
Densidade 1240 kg/m³ ASTM D 792
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 95 - 105 °C -
Pré-secagem - tempo 3 - 5 h -
Umidade do processamento ≤0.02 % -
Temperatura da massa 235 - 265 °C -
Temperatura do molde 80 - 120 °C -
Zona 1 260 - 275 °C -
Zona 2 270 - 285 °C -
Zona 3 280 - 295 °C -
Temperatura do bico 270 - 285 °C -
Características
Processamento
Moldagem por injeção
Características especiais
Retardante de chama, Sem halogéneo, Alto impacto.
Aplicaciones
Elétrica e Eletrônica, Polivalente
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com