Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Luran® S 776SE - ASA - INEOS Styrolution

Material Data Center offers the following functions for Luran® S 776SE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, parameters for material models, CAE Interfaces

Check here, which other Luran datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Luran® S 776SE acrylonitrile styrene acrylate (ASA) polymer features high surface quality and good impact strength including enhanced colour fastness. The product delivers superior long-term performance when exposed to UV irradiation and additionally provide excellent chemical resistance. Luran® S 776SE is suitable extrusion applications. It provides good impact toughness and enables matte surface appearance for extruded sheets.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 4 cm³/10min ISO 1133
Temperatura 220 °C -
Carga 10 kg -
Condutividade térmica do fundido 0.17 W/(m K) -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2200 MPa ISO 527
Tensão no escoamento 47 MPa ISO 527
Deformação no escoamento 3.3 % ISO 527
Deformação nominal na ruptura 12 % ISO 527
Resistência ao impacto Charpy , +23°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 30 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 4 kJ/m² ISO 179/1eA
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 96 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 101 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 92 °C ISO 306
Flamabilidade a 1.5mm esp. nom. HB class IEC 60695-11-10
Espessuras do tubo de teste 1.5 mm -
Cartão Amarelo (yellow card) disponível sim - -
Flamabilidade a espessura h HB class IEC 60695-11-10
Espessuras do tubo de teste 3.0 mm -
Flamabilidade conforme índice de oxigênio 19 % ISO 4589-1/-2
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 1.65 % Sim. to ISO 62
Absorção de umidade 0.35 % Sim. to ISO 62
Densidade 1070 kg/m³ ISO 1183
Diagrama
Tensão - deformação , Luran® S 776SE, ASA, INEOS Styrolution
Módulo secante - deformação , Luran® S 776SE, ASA, INEOS Styrolution
Tensão - deformação (isocrônico) 23°C, Luran® S 776SE, ASA, INEOS Styrolution
Módulo de fluência - tempo 23°C, Luran® S 776SE, ASA, INEOS Styrolution
Curva de fluencia 23°C, Luran® S 776SE, ASA, INEOS Styrolution
Tensão - deformação (isocrônico) 40°C, Luran® S 776SE, ASA, INEOS Styrolution
Módulo de fluência - tempo 40°C, Luran® S 776SE, ASA, INEOS Styrolution
Curva de fluencia 40°C, Luran® S 776SE, ASA, INEOS Styrolution
Tensão - deformação (isocrônico) 60°C, Luran® S 776SE, ASA, INEOS Styrolution
Módulo de fluência - tempo 60°C, Luran® S 776SE, ASA, INEOS Styrolution
Curva de fluencia 60°C, Luran® S 776SE, ASA, INEOS Styrolution
Tensão - deformação (isocrônico) 80°C, Luran® S 776SE, ASA, INEOS Styrolution
Módulo de fluência - tempo 80°C, Luran® S 776SE, ASA, INEOS Styrolution
Curva de fluencia 80°C, Luran® S 776SE, ASA, INEOS Styrolution
Volume específico - temperatura (pvT) , Luran® S 776SE, ASA, INEOS Styrolution
Módulo de tração - temperatura , Luran® S 776SE, ASA, INEOS Styrolution
Características
Processamento
Extrusão de perfis, Extrusão de chapas, Outros tipos de extrusão, Moldagem por sopro, Termoformagem
Forma de entrega
Granulos
Características especiais
Estável a luz, Estabilidade a raios U.V./Intempéries, Estável contra o calor
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Outras informações
Moldagem por injeção
Outros tipos de extrusão
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Pipes, Melt temperature: 200 - 240°C

Extrusão de perfis
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Profiles, Melt temperature: 240°C

Extrusão de chapas
PREPROCESSING

Pre-drying, Temperature: 80°C

Pre-drying, Time: 2 - 4h

PROCESSING

Extrusion, Plates, Melt temperature: 210 - 250°C

Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.