Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® 2405 RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® 2405 RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
  • MVR (300 °C/1.2 kg) 19 cm³/10 min
  • general purpose
  • low viscosity
  • easy release
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 19 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Índice de fluidez, MFI 20 g/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.7 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.7 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2400 MPa ISO 527
Tensão no escoamento 65 MPa ISO 527
Deformação no escoamento 6 % ISO 527
Deformação nominal na ruptura >50 % ISO 527
Módulo de flexão, 23°C 2350 MPa ISO 178
Resistência à flexão 97 MPa ISO 178
Módulo de tensão de fluência, 1h 2200 MPa ISO 899-1
Módulo de tensão de fluência, 1000h 1900 MPa ISO 899-1
Resistência ao impacto Charpy , +23°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, 3mm 65 kJ/m² ISO 179/1eA
Type of failure P - -
Res. impacto Charpy c/entalhe, -30°C, 3mm 14 kJ/m² ISO 179/1eA
Type of failure C - -
Impacto Izod com entalhe, +23°C 65 kJ/m² ISO 180/1A
Impacto Izod com entalhe 15 kJ/m² ISO 180/1A
Temperatura -30 °C -
Perfuração - força máxima, +23°C 5100 N ISO 6603-2
Perfuração - força máxima, -30°C 6000 N ISO 6603-2
Energia de perfuração, +23°C 55 J ISO 6603-2
Energia de perfuração, -30°C 65 J ISO 6603-2
Ball indentation hardness 115 MPa ISO 2039-1
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temp. de transição vítrea, 10°C/min 144 °C ISO 11357-1/-2
Temperatura de deflexão térmica, 1.80 MPa 124 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 137 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 145 °C ISO 306
Coef. de expansão térmica linear, paralelo 65 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 65 E-6/K ISO 11359-1/-2
Flamabilidade a espessura h V-2 class IEC 60695-11-10
Espessuras do tubo de teste 0.8 mm -
Flamabilidade conforme índice de oxigênio 27 % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 875 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 930 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (2) 1 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (3) 1.5 mm -
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Constante dielétrica, 100Hz 3.1 - IEC 62631-2-1
Constante dielétrica, 1MHz 3 - IEC 62631-2-1
Fator de dissipação dielétrica, 100Hz 5 E-4 IEC 62631-2-1
Fator de dissipação dielétrica, 1MHz 90 E-4 IEC 62631-2-1
Resistividade volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividade superficial específica >1E15 Ohm IEC 62631-3-2
Resistência elétrica 34 kV/mm IEC 60243-1
Índice comparativo de linha de fuga 250 - IEC 60112
Propriedades ópticasValorUnidadeMétodo de ensaio
ISO Data
Haze 80 - ISO 14782
Transmitância luminosa 89 % ISO 13468-1, -2
Outras propriedadesValorUnidadeMétodo de ensaio
Absorção de água 0.3 % Sim. to ISO 62
Absorção de umidade 0.12 % Sim. to ISO 62
Densidade 1200 kg/m³ ISO 1183
Bulk density 660 kg/m³ -
Propriedades do filmeValorUnidadeMétodo de ensaio
ISO Dados
WVTR, 23°C/85%r.h. 15 g/(m²*d) ISO 15106-1/-2
Espessura de corpo de prova 0.1 mm -
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 280 °C ISO 294
Moldagem por injeção, temperatura do molde 80 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 120 °C -
Pré-secagem - tempo 2 - 3 h -
Umidade do processamento ≤0.02 % -
Temperatura da massa 280 - 320 °C -
Temperatura do molde 80 - 120 °C -
Zona 1 250 - 260 °C -
Zona 2 270 - 280 °C -
Zona 3 280 - 290 °C -
Temperatura do bico 290 - 300 °C -
Contrapressão 5 - 15 MPa -
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Aditivos
Desmoldante
Características especiais
Transparente, Opaque, Translucent
Certifications
Contém recursos renováveis, ISCC Plus
Aplicaciones
Polivalente
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.