Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® FR6005 - PC FR - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® FR6005:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
  • MVR (300 °C/1.2 kg) 9.0 cm³/10 min
  • medium viscosity
  • easy release
  • flame retardant
  • impact modified
  • good surface quality
  • electrical/electronic
  • housing parts
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 9 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.7 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.7 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2300 MPa ISO 527
Tensão no escoamento 62 MPa ISO 527
Deformação no escoamento 6 % ISO 527
Deformação nominal na ruptura >50 % ISO 527
Módulo de flexão, 23°C 2400 MPa ISO 178
Resistência à flexão 90 MPa ISO 178
Res. impacto Charpy c/entalhe, +23°C 68 kJ/m² ISO 179/1eA
Type of failure P - -
Res. impacto Charpy c/entalhe, -30°C 20 kJ/m² ISO 179/1eA
Type of failure C - -
Impacto Izod com entalhe, +23°C 60 kJ/m² ISO 180/1A
Impacto Izod com entalhe 15 kJ/m² ISO 180/1A
Temperatura -30 °C -
Perfuração - força máxima, +23°C 5100 N ISO 6603-2
Perfuração - força máxima, -30°C 6100 N ISO 6603-2
Energia de perfuração, +23°C 54 J ISO 6603-2
Energia de perfuração, -30°C 55 J ISO 6603-2
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 121 °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 136 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 142 °C ISO 306
Coef. de expansão térmica linear, paralelo 70 E-6/K ISO 11359-1/-2
Coef. de expansão térmica linear, perpend. 70 E-6/K ISO 11359-1/-2
Flamabilidade a 1.5mm esp. nom. V-0 class IEC 60695-11-10
Espessuras do tubo de teste 1.5 mm -
Cartão Amarelo (yellow card) disponível sim - -
Flamabilidade a espessura h V-0 class IEC 60695-11-10
Espessuras do tubo de teste 1.0 mm -
Cartão Amarelo (yellow card) disponível sim - -
Glow Wire Flammability Index (GWFI) 850 °C IEC 60695-2-12
GWFI - thickness tested (1) 1 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 875 °C IEC 60695-2-13
GWIT - thickness tested (1) 1 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 900 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Propriedades elétricasValorUnidadeMétodo de ensaio
ISO Dados
Resistividade volumétrica específica >1E13 Ohm*m IEC 62631-3-1
Resistividade superficial específica >1E15 Ohm IEC 62631-3-2
Índice comparativo de linha de fuga 200 - IEC 60112
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1200 kg/m³ ISO 1183
Produção de amostra para testeValorUnidadeMétodo de ensaio
ISO Dados
Moldagem por injeção, temperatura da massa 300 °C ISO 294
Moldagem por injeção, temperatura do molde 80 °C ISO 294
Moldagem por injeção, velocidade de injeção 200 mm/s ISO 294
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 120 °C -
Pré-secagem - tempo 2 - 3 h -
Umidade do processamento ≤0.02 % -
Temperatura da massa 280 - 320 °C -
Temperatura do molde 80 - 120 °C -
Zona 1 250 - 260 °C -
Zona 2 270 - 280 °C -
Zona 3 280 - 290 °C -
Temperatura do bico 290 - 300 °C -
Contrapressão 5 - 15 MPa -
Características
Processamento
Moldagem por injeção
Forma de entrega
Negro
Aditivos
Desmoldante
Características especiais
Retardante de chama, Alto impacto., Transparente
Aplicaciones
Elétrica e Eletrônica, Encapsulamento
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.