Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Makrolon® LED5902 FR RE - PC - Covestro Deutschland AG

Material Data Center offers the following functions for Makrolon® LED5902 FR RE:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Makrolon datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 6 cm³/10min ISO 1133
Temperatura 300 °C -
Carga 1.2 kg -
Contração após a moldagem, paralelo 0.7 % ISO 294-4, 2577
Contração após a moldagem, perpendicular 0.7 % ISO 294-4, 2577
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 2300 MPa ISO 527
Tensão no escoamento 66 MPa ISO 527
Deformação no escoamento 6.2 % ISO 527
Deformação nominal na ruptura >50 % ISO 527
Tensão na ruptura 60 MPa ISO 527
Deformação na ruptura 60 % ISO 527
Módulo de flexão, 23°C 2400 MPa ISO 178
Resistência à flexão 99 MPa ISO 178
Resistência ao impacto Charpy, +23°C N kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C, 3mm 32 kJ/m² ISO 179/1eA
Impacto Izod com entalhe, +23°C 50[1] kJ/m² ISO 180/1A
Perfuração - força máxima, +23°C 5100 N ISO 6603-2
Perfuração - força máxima, -30°C 6100 N ISO 6603-2
Energia de perfuração, +23°C 50 J ISO 6603-2
Energia de perfuração, -30°C 55 J ISO 6603-2
Ball indentation hardness 120 MPa ISO 2039-1
1: 3 mm
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 121 °C ISO 75-1/-2
Temperatura de deflexão térmica , 0.45 MPa 136 °C ISO 75-1/-2
Temperatura de amolecimento Vicat, B 142 °C ISO 306
Flamabilidade a espessura h V-0 class IEC 60695-11-10
Espessuras do tubo de teste 1.0 mm -
Flamabilidade 5V a espessura h 5VA class IEC 60695-11-20
Espessuras do tubo de teste 3.0 mm -
Flamabilidade conforme índice de oxigênio 39 % ISO 4589-1/-2
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (1) 0.75 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (2) 1.5 mm -
Glow Wire Flammability Index (GWFI) 960 °C IEC 60695-2-12
GWFI - thickness tested (3) 3 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (1) 0.75 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (2) 1.5 mm -
Glow Wire Ignition Temperature (GWIT) 850 °C IEC 60695-2-13
GWIT - thickness tested (3) 3 mm -
Propriedades ópticasValorUnidadeMétodo de ensaio
ISO Data
Haze 1 - ISO 14782
Transmitância luminosa 89 % ISO 13468-1, -2
Other Standards[S]
Índice de refração 1.58 - ISO 489
S: These properties are reported by the producer according standards that are different to our defaults.
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1200 kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 120 °C -
Pré-secagem - tempo 4 h -
Temperatura da massa 280 - 320 °C -
Temperatura do molde 80 °C -
Características
Processamento
Moldagem por injeção
Aditivos
Desmoldante
Características especiais
Retardante de chama, Estabilidade a raios U.V./Intempéries, Transparente
Certifications
Contém recursos renováveis, ISCC Plus
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul, Oriente/África
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com