Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Nypel® 6235G UN - PA6-GF35 - BASF

Material Data Center offers the following functions for Nypel® 6235G UN:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Nypel datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Nypel 6235G UN is a 35% glass reinforced injection molding grade of PA6. Based on recycled polyamide feedstocks, Nypel 6235G UN offers a balance of mechanical properties with the ability to pigment with a full range of colorants.

Nypel 6235G UN is recommended for lawn and power equipment housings, structural furniture components such as seat frames, and automotive and industrial applications.
Propriedades mecânicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Módulo de tração 10655 / 7205 MPa ISO 527
Tensão na ruptura 169 / 116 MPa ISO 527
Deformação na ruptura 3.6 / 7.6 % ISO 527
Resistência ao impacto Charpy , +23°C 96 / 110 kJ/m² ISO 179/1eU
Resistência ao impacto Charpy, -30°C 93 / 92 kJ/m² ISO 179/1eU
Res. impacto Charpy c/entalhe, +23°C 18 / 23 kJ/m² ISO 179/1eA
Res. impacto Charpy c/entalhe, -30°C 15 / 14 kJ/m² ISO 179/1eA
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de deflexão térmica, 1.80 MPa 207 / * °C ISO 75-1/-2
Temperatura de deflexão térmica, 0.45 MPa 217 / * °C ISO 75-1/-2
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1360 / - kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Pré-secagem - temperatura 80 °C -
Pré-secagem - tempo 4 h -
Temperatura da massa 270 - 290 °C -
Temperatura do molde 80 - 90 °C -
Características
Processamento
Moldagem por injeção
Certifications
Conteúdo de resina reciclada
Aplicaciones
Automóvel
Disponibilidade regional
América do Norte
Outras informações
Moldagem por injeção
PREPROCESSING
Pre/Post-processing, Pre-drying, Temperature: 80 °C
Pre/Post-processing, Pre-drying, Time: 4 h

PROCESSING
injection molding, Melt temperature, range: 270 - 290 °C
injection molding, Melt temperature, recommended: 280 °C
injection molding, Mold temperature, range: 80 - 90 °C
injection molding, Mold temperature, recommended: 80 °C
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.