Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox. Information about Biopolymers, a project by FH Hannover and M-Base Engineering & Software GmbH sponsored by Fachagentur Nachwachsende Rohstoffe (FNR).

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of PHARMALENE® MR 50 PH BCA - (PE-LLD) - Versalis S.p.A

Material Data Center offers the following functions for PHARMALENE® MR 50 PH BCA:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Pharmalene datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Pharmalene MR 50 PH BCA will be bio attributed for 90%.
Características de processamento/físicasValorUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez, MFI 22 g/10min ISO 1133
Temperatura 190 °C -
Carga 2.16 kg -
Propriedades mecânicasValorUnidadeMétodo de ensaio
ISO Dados
Tensão no escoamento 15 MPa ISO 527
Tensão na ruptura 15 MPa ISO 527
Deformação na ruptura 450 % ISO 527
Módulo de flexão, 23°C 500 MPa ISO 178
Dureza Shore D 56 - ISO 7619-1
Propriedades térmicasValorUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 126 °C ISO 11357-1/-3
Temperatura de amolecimento Vicat , A 113 °C ISO 306
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 939 kg/m³ ISO 1183
Recomendação de processamento Moldagem por injeçãoValorUnidadeMétodo de ensaio
Temperatura do molde 10 - 40 °C -
Zona 1 170 - 230 °C -
Características
Processamento
Moldagem por injeção
Forma de entrega
Granulos
Resistência Química
Resistência à oxidação
Certifications
Contém recursos renováveis, Contacto com alimentos, Aprovação para contacto com alimentos10/2011, Aprovação de alimentos FDA 21 CFR, Grau médico, USP Class VI, ISCC Plus
Aplicaciones
Médico, Embalaje
Disponibilidade regional
Europa
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.