Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Platamid® H 2707 Pellets - PA* - ARKEMA

Material Data Center offers the following functions for Platamid® H 2707 Pellets:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Platamid datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Informação do produto
Platamid® H 2707 Pellets
Copolyamide Hot Melt Adhesive / Extrusion Applications

Platamid® H 2707 is a standard thermoplastic copolyamide hot melt adhesive available in pellet form. This medium to high melt viscosity grade is particularly suitable for manufacturing webs, mono- and multi-filaments, and films by extrusion.


Platamid® H 2707 offers a good adhesion at low fusing conditions to various polar substrates (thermoplastics, thermosets, metal, natural fibers, etc.).


According to ASTM D6866, the biobased carbon content is measured at 20%.



AVAILABLE GRADES
This grade is available:
- dried (H 2707 T)
PACKAGING
- Platamid® H 2707 T is delivered in 25 kg sealed bags.
SHELF LIFE
Two years from the date of delivery. For any use above this limit, please refer to our technical services.
RENEWABLE CARBON CONTENT
20% (according ASTM D6866)
Características de processamento/físicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Índice de fluidez volumétrico, MVR 2 / * cm³/10min ISO 1133
Temperatura 160 / * °C -
Carga 2.16 / * kg -
Propriedades térmicasSeco / CondUnidadeMétodo de ensaio
ISO Dados
Temperatura de fusão, 10°C/min 102 / * °C ISO 11357-1/-3
Outras propriedadesSeco / CondUnidadeMétodo de ensaio
Densidade 1060 / 1060 kg/m³ ISO 1183
Biobased content 20 % -
Características
Processamento
Extrusão de laminas
Forma de entrega
Granulos
Características
Boa adesão, Copolímero
Certifications
Contém recursos renováveis
Aplicaciones
Monofilament, Multifilament
Disponibilidade regional
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.