Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Premi-Ject® 1100V-10 - UP-GF - LyondellBasell Industries

Material Data Center offers the following functions for Premi-Ject® 1100V-10:
unit conversion, PDF datasheet print, comparison with other plastics

Check here, which other Premi-Ject datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Propriedades mecânicasValorUnidadeMétodo de ensaio
ASTM Dados
Módulo de tração 13790 MPa ASTM D 638
Resistência à tração 31 MPa ASTM D 638
Módulo de flexão 9653 MPa ASTM D 790
Resistência à flexão 72.4 MPa ASTM D 790
Impacto Izod com entalhe, 1/8 in 187 J/m ASTM D 256
Propriedades térmicasValorUnidadeMétodo de ensaio
ASTM Dados
UL94 flamabilidade V-0 - UL 94
Espessuras do tubo de teste 1.52 mm -
Propriedades elétricasValorUnidadeMétodo de ensaio
ASTM Dados
Resistência elétrica, tempo curto 15.7 kV/mm ASTM D 149
Resistência ao arco 180 s ASTM D 495
Outras propriedadesValorUnidadeMétodo de ensaio
Densidade 1800 kg/m³ ASTM D 792
Características
Processamento
Moldagem por injeção, Moldagem por compressão
Forma de entrega
Composto de moldagem em massa
Aditivos
Anti-chama
Características especiais
Retardante de chama, Sem halogéneo, Estável contra o calor
Aplicaciones
Elétrica e Eletrônica
Disponibilidade regional
América do Norte, Europa, Ásia Pacífico, America Centra e do Sul
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.